Process for making opaque polyester film
Abstract
The invention relates to a process for making an opaque and glossy film from a thermoplastic polyester composition, comprising the steps of a) extruding the polyester composition through a slot die, and quenching to form a substantially amorphous film having a crystallinity of at most 5%; b) rapidly heating the amorphous film to a drawing temperature in the range from T g to (T g +50)° C. while applying a draw ratio in the range of from λ initiation to λ max. in longitudinal direction, and a drawing rate of at least 1 m/min to form an oriented film showing stress-whitening, wherein λ initiation is the draw ratio at which a transfer from a transparent product to a stress-whitened product occurs and λ max. is the draw ratio at which failure of the stress whitened film occurs; and c) heat-setting the oriented stress-whitened film; the thermoplastic polyester composition substantially consisting of at least one crystallizable polyester derived from at least one aliphatic diol and at least one aromatic dicarboxylic acid. With this process it is possible to make a unitary, glossy, opaque film from a polyester composition that does not contain void-forming additives like high amounts of f
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 39 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for making an opaque and glossy film from a thermoplastic polyester composition, comprising the steps of a) extruding the polyester composition through a slot die, and quenching to form a substantially amorphous film having a crystallinity of at most 5%; b) heating the amorphous film to a drawing temperature in the range of from 80 to 95° C. by immersing the film in a liquid heating bath, while applying a draw ratio in the range of 5.1 to 5.7 in longitudinal direction using sets of feed and draw rollers the speed of which can be controlled in such a way that speed fluctuations of at
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (39)
Non-Patent Literature (5)
- Bashir et al.; "Evaluation of Three Methods for the Measurement of Crystallinity of PET Resins, Performs, and Bottles"; Polymer Engineering and Science; vol. 40, No. 11; Nov. 2000; pp. 2442-2455.
- Chandran, Prashant et al.; Biaxial Orientation of Poly(ethylene Terephthalate);Adv Polymer Tech, vol. 12, No. 2, 133-151 (1993).
- De et al.; "The Crystal Structure of Polyethylene Terephthalate"; Proceedings of the Royal Society of London; Series A: Mathematical and Physical Sciences; vol. 226; Dec. 7, 1954; 13 Pages.
- Extended European Search Report; European Application No. 080079130.2; Date of Mailing: Aug. 15, 2008; 5 Pages.
- Fakirov et al.; "Unit Cell Dimensions of Poly(ethylene terephthalate)"; Die Makromolekulare Chemie; vol. 176; 1975; 8 Pages.