Dense oxide coated component of a plasma processing chamber and method of manufacture thereof

0Forward Citations (#94314217 Global)
0.0/yrCitation Velocity (#94314217 Global)
0.56Citation PageRank (#94314217 Global)
29Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of forming a dense oxide coating on an aluminum component of semiconductor processing equipment comprises cold spraying a layer of pure aluminum on a surface of the aluminum component to a predetermined thickness. A dense oxide coating is then formed on the layer of pure aluminum using a plasma electrolytic oxidation process, wherein the plasma electrolytic oxidation process causes the layer of pure aluminum to undergo microplasmic discharges, thus forming the dense oxide coating on the layer of pure aluminum on the surface of the aluminum component.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a dense oxide coating on an aluminum component of semiconductor processing equipment comprising: cold spraying a pure aluminum layer on a surface of the aluminum component to a predetermined thickness; and forming a dense oxide coating on the pure aluminum layer using a plasma electrolytic oxidation process, wherein the plasma electrolytic oxidation process causes the pure aluminum layer to undergo microplasmic discharges forming the dense oxide coating on the pure aluminum layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein (a) the pure aluminum layer comprises by weight at least about 99.9% purity and at most about 0.1% incidental impurities; or (b) the pure aluminum layer comprises by weight at least about 99.93% purity and at most about 0.07% incidental impurities.

  3. Claim 3Depends on #1

    The method of claim 1 ,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
US 6,197,178 B1Method for forming ceramic coatings by micro-arc oxidation of reactive metals200188
EP 1,156,130 A1Plasma processing container internal member and production method therefor—23
US 6,365,028 B1Method for producing hard protection coatings on articles made of aluminum alloys200262
US 6,805,952 B2Low contamination plasma chamber components and methods for making the same200491
US 6,808,613 B2Oxidizing electrolytic method for obtaining a ceramic coating at the surface of a metal200415
US 6,896,785 B2Process and device for forming ceramic coatings on metals and alloys, and coatings produced by this process200538
US 6,899,109 B1Method and apparatus for reducing He backside faults during wafer processing200510
US 6,974,523 B2Hollow anode plasma reactor and method200529
US 2006065288 A1Supercritical fluid processing system having a coating on internal members and a method of using—7
US 2007017654 A1Non-oxidizable coating—7
US 7,207,373 B2Non-oxidizable coating200719
US 2007207267 A1Disposable liners for etch chambers and etch chamber components—23
CA 2,540,340 A1Surface modification of aluminum alloy products for micro-arc oxidation processes—9
US 7,291,566 B2Barrier layer for a processing element and a method of forming the same200711
US 7,311,797 B2Productivity enhancing thermal sprayed yttria-containing coating for plasma reactor200732
US 7,396,431 B2Plasma processing system for treating a substrate200824
US 2009200269 A1Protective coating for a plasma processing chamber part and a method of use—102
US 7,605,086 B2Corrosion resistant component of semiconductor processing equipment and method of manufacture thereof20098
US 2011005922 A1Methods and Apparatus for Protecting Plasma Chamber Surfaces—9
US 2011020665 A1Coated metal article and method of manufacturing same—19
US 8,110,045 B2Processing equipment for object to be processed20125
US 2012031765 A1Process for the enhanced corrosion protection of valve metals—36
US 2012103526 A1High purity aluminum coating hard anodization—19
US 8,282,807 B2Metal member having a metal oxide film and method of manufacturing the same20124
US 8,293,335 B2Yttria-coated ceramic components of semiconductor material processing apparatuses and methods of manufacturing the components20125
US 8,313,635 B2Bare aluminum baffles for resist stripping chambers20126
US 8,679,252 B2Actively heated aluminum baffle component having improved particle performance and methods of use and manufacture thereof20143
US 8,728,252 B2Treatment of metal components20144
US 8,888,982 B2Reduction of copper or trace metal contaminants in plasma electrolytic oxidation coatings20144

Non-Patent Literature (5)

  • Blanchard, P.J., "Evaluation of Corrosion Protection Methods for Magnesium Alloys in Automotive Applications", Magnesium Technology, 2005, TMS (The Minerals, Metals & Materials Society), 2005.
  • Curran, J. A. et al., "The Thermal Conductivity of Plasma Electrolytic Oxide Coatings on Aluminium and Magnesium", Surface and Coatings Technology, v. 199 (2-3), pp. 177-183 (2005).
  • Curran, James A., Principal Materials Engineer, "Developments and Approvals on Titanium, Magnesium and Aluminium Composites", Keronite Advanced Surface Technology, ASETSDefense-8th Feb. 2011, pp. 1-33.
  • Dunleavy et al., "Characterisation of discharge events during plasma electrolytic oxidation", Surface and Coatings Technology, 203 (2009), 22: 3410-3419.
  • http://en.wikipedia.org/wiki/Plasma-electrolytic-oxidation for PEO Process, pp. 1-3.