Patents
US 9,541,288 B2#43706309 Most CitedActiveUnited States (USPTO)Utility

Process for operating a furnace with bituminous coal and method for reducing slag formation therewith

2Forward Citations (#43706309 Global)
0.2/yrCitation Velocity (#31816156 Global)
0.92Citation PageRank (#46356024 Global)
24Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

There is provided a process for operating a coal-fired furnace to generate heat. The process has the steps of a) providing the coal to the furnace and b) combusting the coal in the presence of a first slag-reducing ingredient and a second slag-reducing ingredient in amounts effective to reduce slag formation in the furnace. In one embodiment, the first slag-reducing ingredient is one or more oxygenated magnesium compounds and the second slag-reducing ingredient is selected from the group consisting of one or more oxygenated calcium compounds, one or more oxygenated silicon compounds, and combinations thereof. In another embodiment, the first slag-reducing ingredient is one or more oxygenated silicon compounds, and wherein the second slag-reducing ingredient is one or more oxygenated aluminum compounds. There are also provided methods for reducing slag formation in a coal-fired furnace. There are also provided methods for treating coal. There are also treated coals.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for operating a coal-fired furnace, comprising: a) providing coal to a coal-fired furnace; and b) combusting the coal in the presence of a first slag-reducing ingredient and a second slag-reducing ingredient in amounts effective to reduce slag formation in the furnace, wherein the first slag-reducing ingredient is one or more oxygenated magnesium compounds, wherein the second slag-reducing ingredient is one of one or more oxygenated silicon compounds and a combination of one or more oxygenated compounds of aluminum and silicon, wherein the coal exhibits an Si/Al ratio of 2.19 to 2.85

  2. Claim 2Depends on #1

    The process of claim 1 , wherein the one or more oxygenated magnesium compounds is selected from a group consisting of magnesium carbonate, magne

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 2,800,172 AAdditives to fuel195736
US 2,845,338 AFuel additive for removing and inhibiting fireside deposits195821
US 4,280,817 ASolid fuel preparation method198145
DE 3,429,584 A1Combustion-improving additive composition for cleaning heating devices, chimneys, smoke flues and heat regenerators—14
US 4,596,198 ASlag reduction in coal-fired furnaces using oxygen enrichment198626
US 4,654,164 APartial oxidation process198717
US 4,722,610 AMonitor for deposition on heat transfer surfaces198857
US 4,953,481 AMethod for control of slag build-up in solid waste incinerators199017
US 6,165,934 AMaterial and system for catalytic reduction of nitrogen oxide in an exhaust stream of a combustion process200036
JP 2004083796 AFuel additive for preventing slagging trouble and combustion method of fuel—18
US 2006034743 A1Reduction of coal-fired combustion emissions—31
US 2006228282 A1Method for reducing NOx during combustion of coal in a burner—28
US 7,162,960 B2Process for reducing plume opacity200715
US 2007044693 A1Process for improving operation of large-scale combustors—16
US 2007168213 A1Methods of operating a coal burning facility—42
US 7,430,969 B2Method for reducing the amount of a sulfur dioxide in a flue gas resulting from the combustion of a fossil fuel200813
US 2008291965 A1Method for measuring ash/slag deposition in a utility boiler—15
US 2009178599 A1Process for operating a coal-fired furnace with reduced slag formation—16
WO 2009/091539 A1Process for operating a coal-fired furnace with reduced slag formation—5
US 2010006014 A1Targeted reagent injection for slag control from combustion of coals high in iron and/or calcium—8
US 7,775,166 B2Method of using nanoalloy additives to reduce plume opacity, slagging, fouling, corrosion and emissions20105
US 2011269079 A1Process for operating a utility boiler and methods therefor—5
US 8,079,845 B2Processes for operating a utility boiler and methods therefor20113
US 9,127,228 B2Process for operating a furnace with a bituminous coal and method for reducing slag formation therewith20152

Non-Patent Literature (5)

  • Allery et al., "Demonstrated Performance Improvements on Large Lignite-Fired Boiler with Targeted In-Furnace Injection Technology," COAL-GEN 2010; Fuel Tech, Inc., Aug. 10-12, 2010, pp. 1-12.
  • European Patent Office, "Extended European Search Report," European Patent Application No. 12734396.0, dated Feb. 18, 2015, 8 pages.
  • Fuel Tech, Inc., Targeted In-Furnace Injection (TIFI); Oct. 5, 2010, pp. 1-3.
  • International Preliminary Report of Patentability dated Jul. 16, 2013, for International Application No. PCT/US2012/021301, 8 pages.
  • International Search Report dated May 2, 2012, for International Application No. PCT/US2012/021301, 1 page.