US 9,540,544 B2#27265517 Most CitedActiveUnited States (USPTO)Utility

Oxidized mixture of bio-based material and asphalt, a bio-based asphaltic material, and methods of making the same

4Forward Citations (#27265517 Global)
0.4/yrCitation Velocity (#18556585 Global)
1.06Citation PageRank (#38531450 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of forming an asphalt mixture can include mixing a bio-source material and a bitumen source to form a bitumen mixture. The bitumen mixture can be mixed with a catalyst to form the asphalt mixture. Particles can be added to the asphalt mixture to form a roofing-grade asphalt mixture. In an embodiment, the bitumen source material can have a softening point of at least approximately 93° C. and a penetration distance no greater than approximately 25 dmm. In another embodiment, the roofing-grade asphalt mixture can have a softening point of at least approximately 104° C., a penetration distance no greater than approximately 12 dmm, a viscosity of at least approximately 3000 cps at a temperature of 204° C., or any combination thereof. The asphalt mixture can be applied to a base material to form a roofing product. The asphalt mixture can be applied as a pavement product.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming an asphalt mixture comprising: mixing a bitumen source with a bio-source material to form a bitumen mixture, wherein the bio-source material includes an oil, wherein the oil includes recycled cooking oil, recycled vegetable oil, recycled animal fat, or any combination thereof; and adding a liquid catalyst to the bitumen mixture form an asphalt mixture, wherein the liquid catalyst includes a metal salt wherein the metal includes cobalt, manganese, zirconium, vanadium, iron, calcium, nickel, copper, zinc, osmium, rhodium, rhenium, hafnium, or any combination thereof, wherein

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
GB 610,629 AImprovements in or relating to the manufacture of bituminous materials—15
SU 1,133,284 A1Method for producing bitumen19854
US 5,023,282 AAsphalt containing gilsonite, reactive oil and elastomer199138
US 5,494,728 AMethod for making roofing shingles using asphalt fibers, and shingles made thereby199630
US 6,121,440 AProcess for synthesis of polyol fatty acid polyesters200031
US 2005072110 A1Mineral-surfaced roofing shingles with increased solar heat reflectance, and process for producing same—76
EP 1,524,300 A1Polymer-bitumen compositions comprising animal and/or vegetable oils or fats as plasticizers—26
US 7,214,309 B2Process for upgrading heavy oil using a highly active slurry catalyst composition200742
US 7,241,500 B2Colored roofing granules with increased solar heat reflectance, solar heat-reflective shingles, and process for producing same200776
US 2008220167 A1Method of controlling coating edge thickness in a web process—18
US 7,951,417 B1Bio-based adhesive material for roof shingles201126
US 2011244122 A1Bio-based adhesive material—3
US 2011259239 A1Bio-based adhesive material—17
US 8,168,032 B2Method of forming a roofing product including a ceramic base material and recycled roofing material201215
CA 2,799,973 A1Roofing product including roofing-grade asphalt mixture and methods of making the roofing product and the roofing-grade asphalt mixture—7
US 9,181,456 B2Roofing product including roofing-grade asphalt mixture and methods of making the roofing product and the roofing-grade asphalt mixture201515