Patents
US 9,539,701 B2#45343677 Most CitedActiveUnited States (USPTO)Utility

Abrasive article for high-speed grinding operations

2Forward Citations (#45343677 Global)
0.2/yrCitation Velocity (#31910562 Global)
0.86Citation PageRank (#49844497 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An abrasive article includes a bonded abrasive body having abrasive particles comprising microcrystalline alumina (MCA) contained within a bond material. In an embodiment, the bonded abrasive body has a strength ratio (MOR/MOE) of at least about 0.80. Additionally, the bonded abrasive body may have a MOR of at least 40 MPa for a MOE or at least about 40 GPa and the bonded abrasive body may be capable of grinding a workpiece that includes metal at a speed of at least about 60 m/s at a material removal rate of at least about 0.4 in 3 /min/in (258 mm 3 /min/mm).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An abrasive article comprising: a bonded abrasive body having abrasive particles comprising microcrystalline alumina (MCA) contained within a single phase vitreous bond material; wherein the bonded abrasive body comprises: a strength ratio (MOR/MOE) of at least 1.0; a porosity content of at least 42 vol % and not greater than 56 vol % for the total volume of the bonded abrasive body, an abrasive particle content of at least 42 vol % and not greater than 52 vol % for the total volume of the bonded abrasive body; and a bond material content of at least 6 vol % and not greater than 14 vol % for t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,224,380 ATemperature resistant abrasive compact and method for making same1980610
US 4,288,248 ATemperature resistant abrasive compact and method for making same1981263
US 4,314,827 ANon-fused aluminum oxide-based abrasive mineral1982731
US 4,524,138 ASubstantially pore-free sintered polycrystalline articles of α-silicon carbide, boron carbide and free carbon and process for their manufacture198570
US 4,543,107 AVitrified bonded grinding wheels containing sintered gel aluminous abrasive grits1985134
US 4,623,364 AAbrasive material and method for preparing the same1986539
US 4,744,802 AProcess for durable sol-gel produced alumina-based ceramics, abrasive grain and abrasive products1988634
US 4,786,292 AMicrocrystalline abrasive material and method of manufacture198842
US 4,898,597 AFrit bonded abrasive wheel1990133
US 5,035,723 ABonded abrasive products containing sintered sol gel alumina abrasive filaments1991107
US 5,090,970 ABonded abrasive tools with combination of finely microcrystalline aluminous abrasive and a superbrasive199227
US 5,094,672 AVitreous bonded sol-gel abrasive grit article199287
US 5,118,326 AVitrified bonded grinding wheel with mixtures of sol gel aluminous abrasives and silicon carbide199244
US 5,129,919 ABonded abrasive products containing sintered sol gel alumina abrasive filaments199289
US 5,131,923 AVitrified bonded sol gel sintered aluminous abrasive bodies199245
US 5,152,810 ABonded abrasive tools with combination of finely microcrystalline aluminous abrasive and a superabrasive199229
US 5,185,299 AMicrocrystalline alumina-based ceramic articles1993132
US 5,203,886 AHigh porosity vitrified bonded grinding wheels1993141
US 5,203,882 ABonding adjuvants for vitreous bond formulations and process for bonding with199315
US 5,273,558 AAbrasive composition and articles incorporating same1993111
JP H06335866 AVitrified grinding wheel and manufacture thereof—10
US 5,401,284 ASol-gel alumina abrasive wheel with improved corner holding199558
US 5,536,283 AAlumina abrasive wheel with improved corner holding199648
US 5,863,308 ALow temperature bond for abrasive tools199999
WO 9,922,910 A1Low temperature bond for abrasive tools—4
US 6,066,189 AAbrasive article bonded using a hybrid bond200040
US 6,074,278 AHigh speed grinding wheel200055
US 6,086,648 ABonded abrasive articles filled with oil/wax mixture200080

Non-Patent Literature (2)

  • International Search Report from PCT/US2012/031673, dated Oct. 10, 2012, 11 pgs.
  • International Search Report from PCT/US2012/031703, dated Oct. 23, 2012, 12 pgs.