Abstract

Barium, strontium, tantalum and lanthanum precursor compositions useful for atomic layer deposition (ALD) and chemical vapor deposition (CVD) of titanate thin films. The precursors have the formula M(Cp) 2 , wherein M is strontium, barium, tantalum or lanthanum, and Cp is cyclopentadienyl, of the formula wherein each of R 1 -R 5 is the same as or different from one another, with each being independently selected from among hydrogen, C 1 -C 12 alkyl, C 1 -C 12 amino, C 6 -C 10 aryl, C 1 -C 12 alkoxy, C 3 -C 6 alkylsilyl, C 2 -C 12 alkenyl, R 1 R 2 R 3 NNR 3 , wherein R 1 , R 2 and R 3 may be the same as or different from one another and each is independently selected from hydrogen and C 1 -C 6 alkyl, and pendant ligands including functional group(s) providing further coordination to the metal center M. The precursors of the above formula are useful to achieve uniform coating of high dielectric constant materials in the manufacture of flash memory and other microelectronic devices.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a thin film on a substrate, said method comprising contacting the substrate with a vapor of a precursor composition, wherein the precursor composition includes a compound of the formula M(Cp) 2 wherein M(Cp) 2 is bis(tetramethyl-n-propylcyclopentadienyl)strontium, and wherein the compound is not coordinated with letrahydrofuran, to form a thin film comprising strontium on the substrate; and contacting the thin film comprising strontium with an oxidant selected from the group consisting of oxygen, ozone and water.

  2. Claim 2Depends on #1

    The method according to claim 1 , comprising chemical vapor deposition or atomic layer deposition.

  3. Claim 3Depends on #2

    The method according to claim 2 , comprising chemical vapor deposition.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,915,988 AChemical vapor deposition of group IIA metals and precursors therefor199034
US 4,927,670 AChemical vapor deposition of mixed metal oxide coatings1990137
US 4,948,623 AMethod of chemical vapor deposition of copper, silver, and gold using a cyclopentadienyl/metal complex199097
JP H02225317 AProduction of oxide superconductor by chemical gas phase deposition method—15
US 4,960,916 AOrganometallic antimony compounds useful in chemical vapor deposition processes199079
US 4,962,214 ACatalytic enantioselective addition of hydrocarbon equivalents to alpha, beta-unsaturated carbonyl compounds199043
US 5,204,314 AMethod for delivering an involatile reagent in vapor form to a CVD reactor1993372
US 5,204,057 AHighly purified titanium material and its named article, a sputtering target199328
US 5,225,561 ASource reagent compounds for MOCVD of refractory films containing group IIA elements1993180
US 5,280,012 AMethod of forming a superconducting oxide layer by MOCVD1994151
JP H0770747 ATarget material for forming high-purity dielectric thin film—6
JP H07249616 AVapor growth method of dielectric film—14
US 5,453,494 AMetal complex source reagents for MOCVD1995265
US 5,536,323 AApparatus for flash vaporization delivery of reagents1996257
US 5,555,154 ACVD Raw Material for oxide-system dielectric thin film and capacitor produced by CVD method using the CVD raw material199634
US 5,711,816 ASource reagent liquid delivery apparatus, and chemical vapor deposition system comprising same1998243
US 5,721,043 AMethod of forming improved thin film dielectrics by Pb doping19988
JP H10125237 APlasma display panel and its manufacture—43
US 5,770,921 APlasma display panel with protective layer of an alkaline earth oxide199865
US 5,820,664 APrecursor compositions for chemical vapor deposition, and ligand exchange resistant metal-organic precursor solutions comprising same1998253
JP H10273779 ACvd device—12
US 5,837,417 AQuinone diazide compositions containing low metals p-cresol oligomers and process of producing the composition199811
US 5,840,897 AMetal complex source reagents for chemical vapor deposition1998230
US 5,919,522 AGrowth of BaSrTiO3 using polyamine-based precursors1999123
US 6,002,036 AProcess for producing bis(alkyl-cyclopentadienyl)ruthenium complexes and process for producing ruthenium-containing films by using the same199940
US 6,025,222 AVapor phase growth of a dielectric film and a fabrication process of a semiconductor device having such a dielectric film200041
US 6,024,847 AApparatus for producing titanium crystal and titanium200033

Non-Patent Literature (1)

  • Anderson, Q., et al., "Synthesis and Characterization of the First Pentaphenylcyclopentadienyl Copper(I) Complex, (Ph5Cp)Cu(PPh3)", "Organometallics", 1998, pp. 4917-4920, vol. 17.