Patents
US 9,530,535 B2#58977842 Most CitedActiveUnited States (USPTO)Utility

Hydrogen-free amorphous dielectric insulating thin films with no tunneling states

1Forward Citations (#58977842 Global)
0.1/yrCitation Velocity (#46273971 Global)
0.78Citation PageRank (#58977842 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A hydrogen-free amorphous dielectric insulating film having a high material density and a low density of tunneling states is provided. The film is prepared by e-beam deposition of a dielectric material on a substrate having a high substrate temperature T sub under high vacuum and at a low deposition rate. In an exemplary embodiment, the film is amorphous silicon having a density greater than about 2.18 g/cm 3 and a hydrogen content of less than about 0.1%, prepared by e-beam deposition at a rate of about 0.1 nm/sec on a substrate having T sub =400° C. under a vacuum pressure of 1×10 −8 Torr.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for making a high-density amorphous silicon dielectric insulating thin film having no two-level tunneling states (TLS) for a superconducting circuit, comprising: depositing hydrogen-free amorphous silicon on a substrate having a substrate temperature T sub between about 350° and 400° C. the hydrogen-free amorphous silicon being deposited under a high vacuum pressure between about 1×10 −7 and about 1×10 −11 Torr and at a deposition rate of less than 0.1 nm/sec; wherein the substrate temperature, vacuum pressure, and deposition rate are configured to cause the hydrogen-free amorphou

  2. Claim 2Depends on #1

    The process according to claim 1 , wherein

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (5)

  • D.R. Queen, X. Liu, J. Karel, H.C. Jacks, T.H.Metcalf, and F. Hellman, "Two-level systems in evaporated amorphous silicon," Journal of Non-Crystalline Solids 426 (2015) 19-24.
  • D.R. Queen, X. Liu, J. Karel, T.H. Metcalf, and F. Hellman, "Excess specific heat in evaporated amorphous silicon," Phys. Rev. Lett., 110, 135901 (2013).
  • G. L. Pearson and J. Bardeen, "Electrical Properties of Pure Silicon and Silicon Alloys Containing Boron and Phosphorus," Phys. Rev. vol. 75, No. 5, pp. 865-883 (1949).
  • H. Paik and K.D. Osborn, "Reducing quantum-regime dielectric loss of silicon nitride for superconducting quantum circuits," Appl. Phys. Lett., 96, 072505 (2010).
  • H. Paik, D.I. Schuster, L. S. Bishop, G. Kirchmair, G. Catelani, A.P. Sears, B.R. Johnson, M.J. Reagor, L. Frunzio, L.I. Glazman, S.M. Girvin, M.H. Devoret, and R.J. Schoelkop, "Observation of High Coherence in Josephson Junction Qubits Measured in a Three-Dimensional Circuit QED Architecture," Phys