Milling process
Abstract
The invention pertains to a process for cryogenic milling mixtures of (per)fluoroelastomers and semicrystalline thermoplastic VDF polymers, and to free-flowing micronized pellets obtainable therefrom, said micronized pellets advantageously yielding, after extrusion and compounding, excellent mechanical properties, even improved over those of base fluoroelastomer matrix.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 44 · Forward citations: 1.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for manufacturing micronized pellets of a (per)fluoroelastomer composition, said process comprising milling a composition consisting essentially of at least one (per)fluoroelastomer (A) and at least one thermoplastic semicrystalline vinylidene fluoride polymer (F) at a temperature below glass transition temperature of said (per)fluoroelastomer, wherein the micronized pellets, after 24 hours of storage at room temperature, have a pourability of less than 60 s when measured according to ASTM D1895 standard, using the funnel of Test method B and the cylinder of Test Method A, when measu
- Claim 2Depends on #1
The process of claim 1 , wherein fluoroelastomer (A) is selected from the group consisting of: (1) VDF-based copolymers, in which VDF is copolymerized with at least one comonomer selected from the group cons
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| WO 2023/285511 A1 | Binder composition for secondary batteries | — | 5 |
References Cited — Backward Prior Art (44)
Non-Patent Literature (2)
- Standard ASTM D1895-96, "Standard Test Methods for Apparent Density, Bulk Factor, and Pourability of Plastic Materials", 1996 (Reapproved 2010), 5 pages.
- Standard ASTM D3418-08 "Standard test method for transition temperatures and enthalpies of fusion and crystallization of polymers by differential scanning calorimetry", 2008, 7 pages.