Material for joining and product produced therewith
Abstract
The invention relates to an iron-based brazing material comprising a brazing alloy, which alloy comprises: from about 9 wt % to about 30 wt % Cr, from about 5 wt % to about 25 wt % Ni, from about 0 wt % to about 9 wt % Mo, from about 0 wt % to about 5 wt % Mn, from about 0 wt % to about 1 wt % N, from about 6 wt % to about 20 wt % Si. Within the alloy is at least one of the B and the P are present as a melting point lowering supplement to Si, and wherein B is from about 0.1 wt % to about 1.5 wt %, or wherein P is from about 0.1 to about 15 wt % P. The brazing alloy may comprise contaminating elements as at least one of C, O, and S, and optionally the brazing alloy also comprises at least one micro-alloying element as V, Ti, W, Nb, or Ta, and the micro-alloying element is less than 1.5 wt % in the brazing alloy. All values are stated in weight percent, and wherein Si, B and P lower the liquidus temperature, that is the temperature when the brazing material is completely melted.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An iron-based brazing material comprising an iron-based braze filler alloy consisting of: from 9 wt % to 30 wt % Cr; from 5 wt % to 25 wt % Ni; from 0.5 wt % to 9 wt % Mo; from 1 wt % to 5 wt % Mn; from 0 wt % to 1 wt % N; from 8 wt % to 20 wt % Si; wherein the braze alloy also consists of from 0.1 wt % to 1.5 wt % B; and contaminating elements as at least one of C, O, and S; and optionally the braze filler alloy also consists of at least one micro-alloying element as V, Ti, W, Nb, or Ta, and the micro-alloying element is less than 1.5 wt % in the braze filler alloy; and wherein the alloy is b
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Bolton et al, Silicide Phase Formation and its Influence on Liquid Phase Sintering in 316L Stainless Steel with Elemental Silicon Additions, Powder Metallurgy vol. 41 No. 2, 1998, pp. 93-101.
- Brazing and Soldering, Proceedings of the 4th International Brazing and Soldering Conference, Apr. 26-29, 2009, Hilton in the Walt Disney World Resort, Orlando, Florida, USA, pp. 125-129.
- Brazing, Karlebo Handbook, Chapter 12.3.7 Brazing, Liber Utbildning, 1992, p. 750.
- Eagar, Energy Sources Used for Fusion Welding, p. 3, Schwartz, Fundamentals of Brazing, pp. 114-129 Metals Handbook 10th Edition, vol. 6 Welding and Brazing, American Society for Metals, Dec. 1993.
- First Office Action issued in corresponding Chinese Application No. 201410440864.5, dated Nov. 2, 2015, pp. 1-14.