Graphite particles and lithium secondary battery using the same as negative
Abstract
A method for forming a negative electrode for a lithium secondary battery, includes providing a paste comprising graphite particulates comprise assembled or bound graphite particles in each of which a plurality of flat-shaped particles are assembled or bound together so that the planes of orientation are not parallel to one another, and the mixture including 3 to 10 parts by weight of the organic binder per 100 parts by weight of the graphite particulates, a binder and a solvent, coating the paste on a current collector, drying the paste coated on the current collector to form a mixture of the graphite particulates and the binder, and integrating the mixture with the current collector by pressing to provide a density of the mixture of graphite particulates and organic binder of 1.5 to 1.9 g/cm 3 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A graphite particle, wherein pore volume of the pores having a size falling in the range of 10 2 to 10 6 Å is 0.4 to 2.0 cc/g per weight of graphite particle, and wherein pore volume of the pores having a size falling in the range of 1×10 2 to 2×10 4 Å is 0.08 to 0.04 cc/g per weight of graphite particle.
- Claim 2Depends on #1
A graphite particle according to claim 1 , wherein aspect ratio of the graphite particle is 5 or less.
- Claim 3Depends on #2
A graphite particle according to claim 2 , wherein the size of crystallite in the direction of c-axis (direction of thickness) of crystal is 500 Å or more and the size of crystallite in the direction of plane is 1,000 Å or less, as measured by means of X ray broad angle diffraction of the graphite particle.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 10,601,047 B1 | Pre-cracked anode particles for high-rate charging applications | 2020 | 0 |
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Canadian Office Action dated May 10, 2011.
- Catalytic Graphitization Phenomenon, No. 102, pp. 118-131, 1980, Asao Otani.
- Chemistry and Engineering of Carbon Materials, (p. 212), by: Isao Mochida, published Sep. 10, 1990.
- Chinese Office Action dated Mar. 2, 2012.
- JP Office Action of Appln. No. 2015-035158 dated Aug. 5, 2015.