Silicon wafer and method of manufacturing thereof, and method of manufacturing semiconductor device

2Forward Citations (#45314928 Global)
0.2/yrCitation Velocity (#33562977 Global)
0.87Citation PageRank (#49775234 Global)
16Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An object of the present invention is to provide an epitaxial wafer on which dislocation is preventable even when a LSA treatment is performed in device processes. An epitaxial wafer according to the present invention includes a wafer 11 whose nitrogen concentration is 1×10 12 atoms/cm 3 or more or whose specific resistance is 20 mΩ·cm or less by boron doping, and an epitaxial layer 12 provided on the wafer 11 . On the wafer 11 , if a thermal treatment is performed at 750° C. for 4 hours and then at 1,000° C. for 4 hours, polyhedron oxygen precipitates grow predominantly over plate-like oxygen precipitates. Therefore, in the device processes, plate-like oxygen precipitates cannot be easily formed. As a result, even when the LSA treatment is performed after various thermal histories in the device processes, it is possible to prevent the dislocation, which is triggered by oxygen precipitates, from generating.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 2.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing an epitaxial wafer, the method comprising: forming an epitaxial layer on a silicon wafer, in which a nitrogen concentration is 1×10 12 atoms/cm 3 or more or a specific resistance is 20 mΩ·cm or less by boron doping, to form the epitaxial wafer; and heating the epitaxial wafer by raising a temperature of the epitaxial wafer to a predetermined temperature at a rate of 5 ° C. per minute or more within a temperature range from 800° C. to the predetermined temperature and keeping the predetermined temperature for 5minutes or more, the predetermined temperature being grea

  2. Claim 2Independent Claim

    The method of manufac

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • German Office Action for File No. 11 2011 100 479.6, dated Feb. 24, 2014; along with an English translation thereof.
  • International Preliminary Report on Patentability for PCT/JP2011/052277, mailed Sep. 18, 2012.
  • International Search Report issued with respect to PCT/JP2011/052277, mailed Mar. 29, 2011.
  • Japanese Office Action issued for Application No. 2014-117540, mail date is Jun. 30, 2015.
  • Korea Office action, dated Jul. 8, 2013 along with a partial English translation thereof, in patent family application No. KR20127018331.