Stainless steel alloys, turbocharger turbine housings formed from the stainless steel alloys, and methods for manufacturing the same
Abstract
Disclosed is an ferritic stainless steel alloy that includes, by weight, about 20% to about 22% chromium, about 0% to about 0.5% nickel, about 0.5% to about 1.0% manganese, about 1.0% to about 2.5% silicon, about 1.5% to about 2.2% tungsten, about 1.3% to about 1.8% niobium, about 0.35% to about 0.45% carbon, and a balance of iron. The alloy is suitable for use in turbocharger turbine housing applications for temperature up to about 1050° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
3% to 1.8% niobium; 0.35% to 0.45% carbon; phosphorus at no more than 0.04%; sulfur at not more than 0.03%; and a balance of iron and unavoidable/inevitable impurities.
- Claim 2Depends on #1
The ferritic stainless steel alloy of claim 1 consisting of 20% to 21% chromium.
- Claim 3Depends on #1
The ferritic stainless steel alloy of claim 1 consisting of 0.6% to 0.9% manganese.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (32)
Non-Patent Literature (2)
- EP Extended Search Report for Application No. EP 15154766.8 dated Feb. 2, 2016.
- EP Search Report for Application No. EP 15168776.1 dated Feb. 1, 2016.