Patents
US 9,490,145 B2#30870967 Most CitedActiveUnited States (USPTO)Utility

Removal of surface passivation

3Forward Citations (#30870967 Global)
0.3/yrCitation Velocity (#25715237 Global)
1.19Citation PageRank (#32713663 Global)
29Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods for removing a passivation film from a copper surface can include exposing the passivation film to a vapor phase organic reactant, for example at a temperature of 100° C. to 400° C. In some embodiments, the passivation film may have been formed by exposure of the copper surface to benzotriazole, such as can occur during a chemical mechanical planarization process. The methods can be performed as part of a process for integrated circuit fabrication. A second material can be selectively deposited on the cleaned copper surface relative to another surface of the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for removing a passivation film from a substrate, the method comprising: providing the substrate comprising a passivation film on a metal surface, wherein the passivation film was formed by exposure of the metal surface to a passivation agent comprising a hydrocarbon; and exposing the passivation film to a vapor phase organic reactant at a temperature of 100° C. to 400° C., wherein the passivation film is not exposed to a plasma during exposure of the passivation film to the vapor phase organic reactant.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the vapor phase organic reactant comprises carboxylic acid.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the vapor phase organic reactant comprises formic acid.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
EP 0,469,456 A1Process for producing copper-clad laminate—86
JP H04333900 AVoice encoding device—4
EP 0,880,168 A2System and method of selectively cleaning copper substrate surfaces, in-situ, to remove copper oxides—111
WO 0,245,167 A2Thin films for magnetic devices—87
US 6,482,740 B2Method of growing electrical conductors by reducing metal oxide film with organic compound containing -OH, -CHO, or -COOH2002286
EP 1,340,269 A2Thin films for magnetic devices—64
US 6,679,951 B2Metal anneal with oxidation prevention200489
US 6,878,628 B2In situ reduction of copper oxide prior to silicon carbide deposition200575
US 6,887,795 B2Method of growing electrical conductors200557
US 6,921,712 B2Process for producing integrated circuits including reduction using gaseous organic compounds200575
US 2006019493 A1Methods of metallization for microelectronic devices utilizing metal oxide—49
US 7,067,407 B2Method of growing electrical conductors200652
US 7,084,060 B1Forming capping layer over metal wire structure using selective atomic layer deposition200679
US 7,220,669 B2Thin films for magnetic device200730
US 7,241,677 B2Process for producing integrated circuits including reduction using gaseous organic compounds200728
US 7,405,143 B2Method for fabricating a seed layer20089
KR 100,869,326 B1thin films for magnetic devices20085
US 7,494,927 B2Method of growing electrical conductors200912
JP 4,333,900 B2磁気メモリセル、磁気構造体及び磁気素子の製造方法、並びに磁気構造体用金属層の成長方法20093
US 7,927,942 B2Selective silicide process201112
US 7,955,979 B2Method of growing electrical conductors201110
US 8,293,597 B2Selective silicide process20129
KR 20120120902 AMetal silicide, metal germanide, methods for making the same and nickel thin film depositions—10
US 2013115768 A1Methods for depositing nickel films and for making nickel silicide and nickel germanide—30
US 8,536,058 B2Method of growing electrical conductors20134
WO 2015/047345 A1Forming layers of materials over small regions by selective chemical reaction including limiting encroachment of the layers over adjacent regions—31
US 2015097292 A1Interconnects having sealing structures to enable selective metal capping layers—11

Non-Patent Literature (5)

  • Chen et al., "Highly Stable Monolayer Resists for Atomic Layer Deposition on Germanium and Silicon," Chem. Mater., 2006, vol. 18, pp. 3733-3741.
  • Ghosal et al., "Controlling Atomic Layer Deposition of TiO2 in Aerogels through Surface Functionalization," Chem. Mater., 2009, vol. 21, pp. 1989-1992.
  • King, Sean W., "Dielectric Barrier, Etch Stop, and Metal Capping Materials for State of the Art and Beyond Metal Interconnects," ECS Journal of Solid State Science and Technology, 2015, vol. 4, No. 1, pp. N3029-N3047.
  • Lee et al., "Area-Selective Atomic Layer Deposition Using Self-Assembled Monolayer and Scanning Probe Lithography," Journal of the Electrochemical Society, 2009, vol. 156, No. 9, pp. G125-G128.
  • Low et al., "Selective Deposition of CVD Iron on Silicon Dioxide and Tungsten," Microelectric Engineering, 2006, vol. 83, pp. 2229-2233.