Patents
US 9,490,108 B2#93168272 Most CitedActiveUnited States (USPTO)Utility

Indium target and method for manufacturing same

0Forward Citations (#93168272 Global)
0.0/yrCitation Velocity (#93168272 Global)
0.56Citation PageRank (#93168272 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Provided are an indium target capable of achieving a high deposition rate while suppressing the occurrence of arcing, and a method for manufacturing the indium target. In the process of solidification at the time of melting and casting an indium ingot, ultrasonic vibration is applied to molten indium liquid which is at least in a state immediately before solidification, and thereby, coarsening of the grain size is suppressed. Thus, an indium target is provided An indium target in which an overall average grain size is 10 mm or less; for the grains observed from a cross-section parallel to a thickness direction, a ratio of an average grain size in a direction parallel to the thickness direction with respect to an average grain size in a direction perpendicular to the thickness direction is 0.7 to 1.1; and pores with a pore size of 50 μm or greater exists at a density of 1 pore/cm 3 or less.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A sputtering target consisting of indium at a purity of at least 99.99% by mass, wherein: the target has cast structure; an overall average grain size is 1 to 10 mm; for the grains observed from a cross-section parallel to a thickness direction, a ratio of an average grain size in a direction parallel to the thickness direction with respect to an average grain size in a direction perpendicular to the thickness direction is 0.7 to 1.1; and pores with a pore size of 50 μm or greater exists at a density of 0 pore/cm 3 .

  2. Claim 2Depends on #1

    The sputtering target according to claim 1 , wherein the maximum grain size is 20 mm or less.

  3. Claim 3Depends on #1

    The sputtering target according to claim 1 , wherein the maximum grain size is 5 to 20 mm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,046,651 ASoldering technique196224
US 4,124,474 AMethod and apparatus for controlling the deposition of films by reactive sputtering197827
JP S57185973 AProduction of target for sputtering—22
JP S58145310 AProduction of unevenly walled pipe—7
JP S63111172 AProduction of target material—8
JP S6344820 AProtective sheet for directly protecting plant—29
JP H0399741 AMethod of manufacturing valve—14
US 5,054,195 AProcess for the production of a valve199135
EP 0,500,031 A1Method of manufacturing a sputtering target—48
JP H04301074 ATarget for sputtering—11
JP H05214519 ATitanium sputtering target—18
US 5,269,453 ALow temperature method for forming solder bump interconnections to a plated circuit trace1993142
JP H06287661 AProduction of smelted material of refractory metal—13
JP H0860352 AIto sputtering target—26
JP H08218165 ATarget for indium-tin oxide film—10
JP H08281208 APretreatment for coating of ground part of aluminum alloy—16
JP H0925564 AAluminum or aluminum alloy sputtering target—23
US 5,630,918 AITO sputtering target199744
JP H10280137 AProduction of sputtering target—13
JP H11236664 ABacking plate of target for sputtering—19
US 6,030,514 AMethod of reducing sputtering burn-in time, minimizing sputtered particulate, and target assembly therefor200053
WO 0,173,156 A2Method of forming aluminum targets—14
US 6,309,556 B1Method of manufacturing enhanced finish sputtering targets200116
DE 10,063,383 C1Production of a tubular target used for cathode sputtering devices comprises forming an outer tube by casting a molten material in a mold, in which the mold has a heated core rod formed from an inner tube200219
JP 2003089869 ASputtering target, and production method therefor—12
JP 2003136190 ADie for vibratory casting for manufacturing ingot having fine crystalline particles—9
US 2003089482 A1Process for producing a tube-shaped cathode sputtering target—16
JP 2003183820 ASputtering target—21
JP 2003533589 Aアルミニウムを含んでなる物理蒸着ターゲット;スパッタ膜;及びターゲット構造を形成する方法—14
US 6,719,034 B2Process for producing a tube-shaped cathode sputtering target200430

Non-Patent Literature (5)

  • A Dictionary of Chemistry, Sixth Edition, 2008, p. 283, p. 434, John Daintith, ed., 4 pages.
  • Alloy Digest, Indium Semi-Conductor Grade (data sheet), ASM International, Mar. 1998, 2 pages.
  • English translation of International Preliminary Report on Patentability issued Mar. 25, 2014 in co-pending PCT application No. PCT/JP2012/068838.
  • English translation of International Search Report mailed Aug. 28, 2012 in co-pending PCT application No. PCT/JP2012/068838.
  • English translation of the International Preliminary Report on Patentability transmitted Sep. 12, 2013 in co-pending PCT application No. PCT/JP2011/065585.