Patents
US 9,469,065 B2#115162091 Most CitedActiveUnited States (USPTO)Utility

Process for forming a sheet of thermoplastic material

0Forward Citations (#115162091 Global)
0.0/yrCitation Velocity (#115162091 Global)
0.56Citation PageRank (#115162091 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Provided is a process for forming a sheet of thermoplastic material into a three-dimensional shape, the process comprising the steps of (i) forming the sheet at a temperature below its glass transition temperature to produce a first formed shape in the sheet, followed by (ii) raising the temperature of the first formed shape ( 20 ) to above its glass transition temperature whilst a male former ( 12 ), having at least a portion of its profile being substantially the same as that of the first formed shape ( 20 ), is positioned to substantially align at least a portion of its profile with that of the first formed shape ( 20 ), thereby restricting the first formed shape from shrinking back towards its original sheet form, followed by (iii) further forming the first formed shape ( 20 ) at a temperature below that of the glass transition temperature, to form a second formed shape ( 24 ), followed by (iv) raising the temperature of the second formed shape ( 24 ) to above its glass transition temperature whilst a male former ( 16 ), at least a portion of its profile being substantially the same as that of the second formed shape ( 24 ), is positioned to substantially align at least a porti

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for forming a sheet of thermoplastic material into a three-dimensional shape, the process comprising the steps of: (i) starting with a thermoplastic material having an average thickness of less than about 1.0 mm; (ii) forming the sheet at a temperature below its glass transition temperature to produce a first formed shape in the sheet, followed by (iii) raising the temperature of the first formed shape to above its glass transition temperature, to over 100° C.; while a male former, having at least a portion of its profile being substantially the same as that of the first formed shape

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (2)

  • European Search Report in EP application EP 11 15 9346 dated Oct. 14, 2011 with Written Opinion.
  • PCT International Search Report in PCT application PCT/EP2012/055075 dated Jun. 18, 2012 with Written Opinion.