Patents
US 9,460,918 B2#32516288 Most CitedActiveUnited States (USPTO)Utility

Epitaxy of high tensile silicon alloy for tensile strain applications

3Forward Citations (#32516288 Global)
0.3/yrCitation Velocity (#25808062 Global)
1.10Citation PageRank (#36797988 Global)
22Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the present invention generally relate to methods for forming silicon epitaxial layers on semiconductor devices. The methods include forming a silicon epitaxial layer on a substrate at increased pressure and reduced temperature. The silicon epitaxial layer has a phosphorus concentration of about 1×10 21 atoms per cubic centimeter or greater, and is formed without the addition of carbon. A phosphorus concentration of about 1×10 21 atoms per cubic centimeter or greater increases the tensile strain of the deposited layer, and thus, improves channel mobility. Since the epitaxial layer is substantially free of carbon, the epitaxial layer does not suffer from film formation and quality issues commonly associated with carbon-containing epitaxial layers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a film on a substrate, comprising: positioning a substrate within a processing chamber; heating the substrate to a temperature within a range from about 550 degrees Celsius to about 750 degrees Celsius; introducing process gases into the processing chamber, the process gases consisting of a silicon source, a phosphorus source, and a carrier gas; and depositing a substantially carbon-free silicon epitaxial layer on the substrate, the substantially carbon-free silicon epitaxial layer having a phosphorus concentration of 3×10 21 atoms per cubic centimeter or greater and a ten

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 5,316,958 AMethod of dopant enhancement in an epitaxial silicon layer by using germanium1994129
US 5,700,520 ALow temperature, high pressure silicon deposition method199756
JP H1041321 AManufacture of bipolar transistor—14
US 5,731,626 AProcess for controlling dopant diffusion in a semiconductor layer and semiconductor layer formed thereby1998132
US 6,107,197 AMethod of removing a carbon-contaminated layer from a silicon substrate surface for subsequent selective silicon epitaxial growth thereon and apparatus for selective silicon epitaxial growth200056
US 6,197,666 B1Method for the fabrication of a doped silicon layer200119
US 6,346,452 B1Method for controlling an N-type dopant concentration depth profile in bipolar transistor epitaxial layers200226
US 2003045063 A1Semiconductor device and method for manufacturing the same—60
US 6,579,752 B2Phosphorus dopant control in low-temperature Si and SiGe epitaxy20038
US 2005079691 A1Methods of selective deposition of heavily doped epitaxial SiGe—79
CN 1,875,461 AMethod for selectively depositing heavily doped epitaxial silicon germanium—24
US 7,166,528 B2Methods of selective deposition of heavily doped epitaxial SiGe200759
US 7,176,111 B2Method for depositing polycrystalline SiGe suitable for micromachining and devices obtained thereof200714
US 7,195,985 B2CMOS transistor junction regions formed by a CVD etching and deposition sequence200786
US 2008079691 A1Information processing apparatus, transmitter, and control method—10
US 2008102602 A1Structure of strained silicon on insulator and method of manufacturing the same—5
US 2008169512 A1Non-planar pMOS structure with a strained channel region and an integrated strained CMOS flow—39
US 2008182075 A1Phosphorus Containing Si Epitaxial Layers in N-Type Source/Drain Junctions—23
US 2009026496 A1Methods of making substitutionally carbon-doped crystalline si-containing materials by chemical vapor deposition—8
US 2010224937 A1Method for integrating silicon germanium and carbon doped silicon within a strained cmos flow—25
US 2011147828 A1Semiconductor device having doped epitaxial region and its methods of fabrication—196
US 2014084369 A1Semiconductor device having doped epitaxial region and its methods of fabrication—38

Non-Patent Literature (5)

  • Chinese Office Action dated Jun. 30, 2015 for Application No. 201180066837.0.
  • Chinese Office Action dated Mar. 15, 2016 for Application No. 201180066837.0.
  • Chinese Office Action dated Nov. 19, 2015 for Application No. 201180066837.0.
  • European Search Report dated Oct. 9, 2016 for Application No. 118581628.
  • Huang et al., "Further study on structural and electronic properties of silicon phosphide compounds with 3:4 stoichiometry", Computational Materials Science, Elsevier, Amsterdam, NL, Aug. 2004 vol. 30, No. 3-4, pp. 371-375.