Patents
US 9,446,989 B2#111636945 Most CitedActiveUnited States (USPTO)Utility

Carbon fiber-reinforced article and method therefor

0Forward Citations (#111636945 Global)
0.0/yrCitation Velocity (#111636945 Global)
0.56Citation PageRank (#111636945 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of fabricating a carbon fiber-reinforced article includes providing carbon fibers that have surfaces that include an initial interfacial bonding strength capacity with respect to bonding with boron nitride. The surfaces are then modified to reduce the initial interfacial bonding strength capacity. A layer of boron nitride is then deposited on the modified surfaces and the carbon fibers are then embedded in a ceramic matrix. A carbon fiber-reinforced article includes the carbon fibers, the layer of boron nitride on the surfaces of the carbon fibers, and the ceramic matrix. The article exhibits non-brittle fracture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a carbon fiber-reinforced article, the method comprising: providing a plurality of carbon fibers, the plurality of carbon fibers including surfaces; ordering microstructural stacking faults in a graphitic microstructure of the surfaces of the plurality of carbon fibers; depositing a layer of boron nitride on the surfaces; depositing a silicon-containing layer on the layer of boron nitride: and embedding the plurality of carbon fibers in a ceramic matrix to provide a carbon fiber-reinforced article.

  2. Claim 2Depends on #1

    The method as recited in claim 1 , wherein the ceramic matrix is silicon carbide.

  3. Claim 3Depends on #1

    The method as recited in claim 1 , wherein the surfaces of the plurality of carbon fibers are free of any ceramic coating prior to the depositing of the layer of boron nitride.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
FR 2,401,888 A1Impregnating porous carbon body with refractory material - esp. carbide, boride and/or nitride to improve compressive strength and erosion resistance—54
JP S5777320 ABoronized fiber and its preparation—9
US 4,543,345 ASilicon carbide whisker reinforced ceramic composites and method for making same1985194
US 4,642,271 ABN coating of ceramic fibers for ceramic fiber composites1987174
US 4,752,503 AProcess for the manufacture of a composite material with refractory fibrous reinforcement and ceramic matrix198884
US 4,808,076 ARotor for a gas turbine engine198935
US 4,960,629 AFiber reinforced composite article199015
US 4,994,416 ACeramic composites reinforced with modified silicon carbide whiskers and method for modifying the whiskers199114
US 5,026,604 AComposite material with refractory fibrous reinforcement and ceramic matrix199139
US 5,094,901 AOxidation resistant ceramic matrix composites199261
US 5,110,652 AShaped fiber-reinforced ceramic composite article199233
US 5,132,169 AComposite materials having multidirectional reinforcement textures made essentially of ceramic fibers having a silicon compound base199211
US 5,134,020 AComposite material with multiple interphases between refractory reinforcing fibers and ceramix matrix199232
US 5,188,878 AUnidirectional thin glass prepreg199312
JP H05102778 APiezoelectric component—2
US 5,246,736 AProcess for the manufacture of a refractory composite material protected against corrosion199379
US 5,252,381 AAirfoil with thick trailing edge199321
US 5,275,844 AProcess for forming a crack-free boron nitride coating on a carbon structure199415
US 5,275,984 AFiber coating of unbonded multi-layers for toughening ceramic fiber-matrix composites199416
US 5,296,311 ASilicon carbide reinforced reaction bonded silicon carbide composite199435
US 5,389,450 AComposite materials and methods for making the same199527
US 5,407,740 ACeramic composites with ceramic fibers199528
US 5,427,986 AB-N-Cx hydrid coatings for inorganic fiber reinforcement materials199511
US 5,433,915 AManufacturing method of composite articles from prepregs which avoids internal defects199552
US 5,445,693 AMethod of producing a formable composite material1995104
US 5,476,685 AProcess for the manufacture of a fiber reinforced composite material having a ceramic matrix and preheated carbon fibers199519
US 5,589,115 AMethod for making fiber-reinforced ceramic matrix composite199642
US 5,593,728 AInterface coating for ceramic fibers199724
US 5,682,594 AComposite materials and methods for making the same199745
US 5,707,471 AMethod for making ceramic matrix composites199864

Non-Patent Literature (3)

  • European Search Report for European Patent Application No. 13869440 completed Nov. 19, 2015.
  • International Preliminary Report on Patentability for PCT Application No. PCT/US2013/077376, mailed Jul. 9, 2015.
  • U.S. Appl. No. 13/189,013, filed Jul. 22, 2011. Ceramic composite article having laminar ceramic matrix.