Abstract

The invention relates to the field of ion exchange with the formation of a complex or chelate by using complex-forming polymers and can be used in nonferrous metallurgy and hydrometallurgy of indium for extraction of indium from wastewaters, as well as in the chemical industry and for producing special-purity substances. A method for producing a complex-forming sorbent for selective extraction of indium is proposed, wherein the method comprises the introduction of gem-diphosphonic functional groups, and wherein, in order to increase the selectivity and sorption capacity for indium, the gem-diphosphonic functional groups are introduced by the treatment of a spherically granulated cross-linked macroporous acrylonitrile-divinylbenzene copolymer with phosphorous acid at temperature of from 140 to 160° C. for from 13 to 35 hours. In the presence of a diluent (chlorobenzene), the method is carried out at a temperature of between 100 and 130° C. The technical result is to introduce gem-diphosphonic functional groups by the treatment of spherically granulated cross-linked macroporous acrylonitrile-divinylbenzene copolymer with phosphorous acid, which simplifies the method for production an

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a gem-diphosphonic functional groups-containing, complex-forming sorbent for selective extraction of indium, the method comprising treating a spherically granulated cross-linked macroporous acrylonitrile-divinylbenzene copolymer with dried phosphorous acid at an elevated temperature with following separating and washing product granules with water and ethanol sequentially.

  2. Claim 2Depends on #1

    The method according to claim 1 , characterized in that the treating is carried out in a melt of dried phosphorous acid at a temperature of from 140 to 160° C. for from 13 to 35 hours.

  3. Claim 3Depends on #1

    The method according to claim 1 , characterized in that the treating with dried phosphorous acid is carried out in chlorobenzene at a temperature of from 100 to 130° C. for from 13 to 35 hours.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (2)

  • Feb. 21, 2013-(RU) Search Report-App RU 2012132262 (Russian Priority Document).