Patents
US 9,370,902 B2#41585510 Most CitedActiveUnited States (USPTO)Utility

Fiber-reinforced epoxy composites and methods of making same without the use of oven or autoclave

2Forward Citations (#41585510 Global)
0.2/yrCitation Velocity (#33283590 Global)
0.97Citation PageRank (#43142307 Global)
31Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Method embodiments for producing a fiber-reinforced epoxy composite comprise providing a mold defining a shape for a composite, applying a fiber reinforcement over the mold, covering the mold and fiber reinforcement thereon in a vacuum enclosure, performing a vacuum on the vacuum enclosure to produce a pressure gradient, insulating at least a portion of the vacuum enclosure with thermal insulation, infusing the fiber reinforcement with a reactive mixture of uncured epoxy resin and curing agent under vacuum conditions, wherein the reactive mixture of uncured epoxy resin and curing agent generates exothermic heat, and producing the fiber-reinforced epoxy composite having a glass transition temperature of at least about 100° C. by curing the fiber reinforcement infused with the reactive mixture of uncured epoxy resin and curing agent by utilizing the exothermically generated heat, wherein the curing is conducted inside the thermally insulated vacuum enclosure without utilization of an external heat source or an external radiation source.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a fiber-reinforced epoxy composite comprising: providing a mold defining a shape for a composite; applying a fiber reinforcement over the mold; covering the mold and fiber reinforcement thereon in a vacuum enclosure; performing a vacuum on the vacuum enclosure to produce a pressure gradient; insulating at least a portion of the vacuum enclosure with thermal insulation; infusing the fiber reinforcement with a reactive mixture of uncured epoxy resin and an amine curing agent under vacuum conditions, wherein the reactive mixture of uncured epoxy resin and curing agent gener

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (31)

PatentTitleYearCitations
US 4,167,430 AMethod for fabricating a composite bonded structure197961
GB 2,172,542 AMoulds—34
US 4,936,939 AFabric-reinforced ceramic matrix composite material199059
US 4,944,824 AProcess for preparation of tooling of carbon fiber reinforced polyimide for composites manufacture199031
EP 0,662,492 A1Fire-safe panels, fixtures and laminated honeycomb structures of fiber-reinforced ceramic material—15
US 5,569,508 AResin transfer molding with honeycomb core and core filler199663
WO 0,054,949 A2Heated tooling apparatus and method for processing composite and plastic material—42
US 2002022422 A1Double bag vacuum infusion process and system for low cost, advanced composite fabrication—164
US RE37920 EFlat panel display200225
US 6,752,190 B1Cure-on-the-fly system200428
US 7,192,634 B2Flexible polymer element as toughening agent in prepregs200736
US 2008197526 A1Process for Preparing Composites Using Epoxy Resin Formulations—22
US 2009131556 A1Epoxy resin composition, fiber-reinforced composite material and production method of the same—20
US 2009189320 A1Heat vacuum assisted resin transfer molding processes for manufacturing composite materials—24
US 2009252921 A1Method for the production of a sandwich component having a honeycomb core and the sandwich component obtained in this way—36
US 2010143145 A1Fibre-reinforced composite moulding and manufacture thereof—24
US 2010196654 A1Process for producing composite laminate structures and composite laminate structures formed thereby—11
US 2011077328 A1Use of filler that undergoes endothermic phase transition to lower the reaction exotherm of epoxy based compositions—12
US 2011139344 A1High temperature composite tool—41
US 2011254196 A1Method for making an acoustic attentuation panel, in particular for aeronautics—8
US 8,163,209 B2Method and apparatus for controlling the geometry of a composite component20125
US 8,308,889 B2Out-of-autoclave and alternative oven curing using a self heating tool20126
US 8,356,989 B2Double bag vacuum infusion process and system for low cost, advanced composite fabrication20139
US 2013096232 A1Curable epoxy resin compositions and composites made therefrom—13
WO 2013/075716 A1Curing composite materials comprising latent-cure resins—5
RU 2,488,612 C1Epoxide composition for making articles from polymer composite materials by vacuum infusion201310
US 2013225788 A1Curable resin composition and short-cure method—35
US 8,728,262 B2Rapid fabrication of a composite part20144

Non-Patent Literature (5)

  • "Fabrication Methods (2015)", CompositesWorld, Jan. 9, 2015, http://www.compositesworld.com/articles/fabrication-methods-2015.
  • "Fabrication Methods", CompositesWorld, Jan. 1, 2014, http://www.compositesworld.com/articles/fabrication-methods.
  • Barnell et al., "Evaluation of No-Oven, No-Autoclave Composite Manufacturing", Society for the Advancement of Material and Process Engineering with permission, Open Conference Systems, Long Beach, California May 6-9, 2013, http://www.memberjournal.com/SAMPE/index.php?conference.
  • Dierksen, "Optimization of High Temperature VARTM Process", Final Report, Nanotechnology and Material Systems REU, Summer of 2006, pp. 1-7.
  • Dietsch et al, "No-oven, No-autoclave Composite Tool Fabrication", Society for the Advancement of Material and Process Engineering.