Patents
US 9,347,154 B2#78293578 Most CitedActiveUnited States (USPTO)Utility

Drawn poly(ethyleneterephthalate) fiber, poly(ethyleneterephthalate) tire-cord, their preparation method and tire comprising the same

0Forward Citations (#78293578 Global)
0.0/yrCitation Velocity (#78293578 Global)
0.56Citation PageRank (#78293578 Global)
27Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a drawn PET fiber which has good dimensional stability, thereby increases the high speed driving performance of a tire, a PET tire cord, their preparation methods, and a tire including the same. The drawn PET fiber may includes 90 mol % or more of PET and may be a fiber of which a creep rate is 5.5% or less when the drawn PET fiber is fixed under the initial load of 0.01 g/d and is kept for 24 hours under the load of 0.791 g/d and the temperature of 100° C. Furthermore, the PET tire cord may be a cord of which a creep rate is 4.0% or less when the PET tire cord is fixed under the initial load of 0.01 g/d and is kept for 24 hours under the load of 0.791 g/d and the temperature of 100° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A drawn polyethylene terephthalate (PET) fiber, including 90 mol % or more of PET, wherein a creep rate defined by the following Calculation Formula 1 is 5.5% or less when the drawn PET fiber is fixed under the initial load of 0.01 g/d and is kept for 24 hours under the load of 0.791 g/d and the temperature of 100° C.: Creep rate =( L−L 0)/ L 0 ×100  Calculation Formula 1 wherein L is a length of the drawn PET fiber after keeping it for 24 hours, L0 is a length of the drawn PET fiber when it is fixed under the initial load, wherein the drawn PET fiber is obtained by drawing an undrawn PET fibe

  2. Claim 2Depends on #1

    The drawn PET fiber according to claim 1 , wherein the creep rate after heating the drawn PET fiber

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (27)

PatentTitleYearCitations
US 3,946,100 AProcess for the expeditious formation and structural modification of polyester fibers197657
US 3,966,867 AManufacture of unique polyethylene terephthalate fiber197635
US 4,101,525 APolyester yarn of high strength possessing an unusually stable internal structure197896
JP S6119812 APolyester fiber—13
JP S6269819 APolyester fiber—13
EP 0,311,386 A2High-tenacity conjugated fiber and process for preparation thereof—5
US 4,827,999 APolyester fiber having excellent thermal dimensional _ stability, chemical stability and high _ tenacity and process for the production thereof198945
US 5,049,339 AProcess for manufacturing industrial yarn199123
US 5,102,603 AProcess for manufacturing polyethylene terephthalate industrial yarn199216
US 5,137,670 APolyester fiber and process for manufacture199221
US 5,388,628 APneumatic radial tires including polyester carcass with specified elongation and shrinkage19954
JP H0770819 AProduction of polyester fiber—18
US 5,472,781 AHigh strength polyester filamentary yarn199524
US 5,558,935 APolyester fiber and method of manufacturing the same199624
US 5,894,875 APneumatic radial tire with flat 1×6 steel belt cord199925
US 2001039988 A1Polyester multifilamentary yarn for tire cords, dipped cord and production thereof—14
US 2003207111 A1Dimensionally stable polyester yarn for high tenacity treated cords—9
US 6,764,623 B2Process of making polyester filamentary yarn for tire cords200421
KR 20050012625 AA high strength low shrinkage polyester drawn yarn—3
KR 20050020885 APolyethylene terephthalate fibers using stress-strain curve, and process for preparing the same—11
US 6,967,058 B2Polyester multifilament yarn for rubber reinforcement and method of producing the same20058
KR 100,571,214 B1Polyester multifilamentary yarn for tire cords, dipped cord and production thereof200611
KR 100,602,286 B1Polyester fiber and preparation thereof20065
JP 2006188796 AMethod for producing polyester fiber for rubber reinforcement—6
JP 2007022366 APneumatic tire—8
WO 2008/156333 A1Drawn poly(ethyleneterephthalate) fiber, poly(ethyleneterephthalate) tire-cord, their preparation method and tire comprising the same—25
JP 2010530480 Aポリエチレンテレフタレート延伸糸、ポリエチレンテレフタレートタイヤコード、これらの製造方法、およびこれを含むタイヤ—9

Non-Patent Literature (2)

  • European Patent Office, Communication dated Jan. 13, 2015 in corresponding European application No. 08766487.6.
  • Japanese Patent Office, Japanese Office Action issued in corresponding JP Application No. 2010-513125, dated Sep. 25, 2012.