Abstract

An alkali metal ion source with a moderate rate of release of the ion (e.g. potassium) is formed by a method that includes: 1) combining an particulate ore that contains at least one of an alkali metal ion-bearing framework silicate (e.g. syenite ore) with at least one of an oxide and hydroxide of at least one of an alkali metal and alkaline earth metal such as calcium hydroxide; 2) milling the mixture of these two components optionally, with water, optionally, milling the dry components separately and blended thereafter, optionally, with water; 3) forming a mixture by adding water to the solid mixture after milling, if water was not added before milling; 4) exposing the mixture to an elevated temperature and pressure to form a gel that includes silica and the alkali metal of the framework silicate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming an alkali metal ion source with a moderate rate of the ion release, comprising the steps of: a) combining a first component particulate alkali metal ion-bearing framework silicate with a second component that includes at least one of an oxide and a hydroxide of at least one of an alkaline earth metal and an alkali metal to form a solid mixture, wherein the molar ratio of the silicon to the at least one of the alkaline earth metal and alkali metal of the second component in the solid mixture is in a range of between about 1.0:0.1 and about 1.0:0.3; and b) exposing the solid

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the alkali metal of the first co

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (27)

PatentTitleYearCitations
FR 527,066 AProcédé pour la fabrication du carbonate de potassium19212
GB 195,084 AImproved method of treating leucite or other sodium-potassium silicates, for recovering potassium, sodium and aluminium compounds—2
FR 556,994 AMéthode de traitement de la leucite par la chaux pour obtenir de la potasse caustique et un résidu propre à la fabrication du ciment19232
FR 693,074 APerfectionnements aux procédés servant à extraire de la leucite la potasse et l'alumine19302
GB 342,617 AProcess of extracting potash and alumina from leucite—2
US 3,137,564 AProcess for producing a silica gel fertilizer and the product thereof196412
DD 142,802 A3Verfahren zur herstellung einer naehrstoffreichen bodenverbessernden organischen substanz—5
US 4,493,725 AFertilizer product with sustained action and process therefor198535
EP 0,058,922 B1Metallurgical process for treating silicon-aluminous-alkaline ores, in particular leucitic ores19853
US 4,810,280 AMethod for enhancing water retention in soil198927
CN 1,064,262 AProcessing method with producing potassium fertilizer from potash feldspar—4
CN 1,098,398 AA kind of method of producing potash fertilizer by potassium felspar sand—8
US 5,433,766 ASlow-release fertilizer199553
US 5,695,542 AMethod of preparing a slow release fertilizer199720
US 5,858,320 AProcess for preparing ultrafine aluminum silicate salt particles199911
CN 1,365,958 AProcess for preparing K fertilizer (K salt) from K-enriched rock and lime by hydrothermal method—14
CN 1,365,957 AProcess for preparing K fertilizer or K salt from K-enriched rock and lime by hydrothermal method—22
CN 1,508,092 AMethod for preparing potash manure (kali salt) from potassium-rich rock using hydrothermal chemical reaction—26
US 6,887,828 B2Phillipsitic zeolite soil amendments200510
US 7,252,697 B2Methods for making controlled-release ammonium phosphate fertilizer20076
CN 101,054,313 AMethod for producing micro-pore silicon-potassium-calcium mineral fertilizer—12
WO 2009/070953 A1Method for preparing microporous mineral fertilizer from silicates rock using hydrothermal chemical reaction—8
US 2011002870 A1Composition of a material with a porous structure comprising a silicate and a carbonate, hydroxide or oxide of alkaline or alkalinoterrous elements, and corresponding preparation methods and uses—9
WO 2013/044016 A2Geopolymer resin materials, geopolymer materials, and materials produced thereby—34
CN 102,030,338 BMethod for hydrothermally synthesizing kalsilite by using potassium feldspar powder20133
WO 2013/061092 A1Potash product and method—7

Non-Patent Literature (5)

  • Askegaard, M., et al., "A cation exchange resin method for measuring long-term potassium release rates from soil", An International Journal on Plant-Soil Relationships (Kluwer Academic Publishers), 271(1-2): 63-74 (Apr. 1, 2005).
  • Bakken, A.K. et al., "Plant available potassium in rocks and mine tailings with biotite, nepheline and K-feldspar as K-bearing minerals", Acta Argriculturae Scandinavica, Section B-Soil & Plant Science, 47(3) (1997).
  • De Vynck, I.A., "Cristallisation Hydrothermale De Gels Alumino-Silicates Et Magnesio-Silicates En Presence D'Hydroxyde De Calcium", Bullet Des Scoietes Chimiques Belges, 88(12): 989-1002 (Jan. 1, 1979).
  • Gu, Ying-Ying, et al., "Research on the New Technology of activated roasting-acid leaching of potash feldspar", Multipurpose Utilization of Mineral Resources (Jan. 2012).
  • Han, Xiao-Zhao, et al. "Extraction of potassium from potash feldspar ores with sodium chloride", Industrial Minerals and Processing (Sep. 2005).