High impact resistant degradation element
Abstract
In one aspect of the invention, a degradation element includes a substrate bonded to a sintered polycrystalline ceramic. The sintered polycrystalline ceramic has a tapering shape and a rounded apex. The rounded apex has a curvature with a 0.050 to 0.150 inch radius when viewed from a direction normal to a central axis of the degradation element that intersects the curvature. The rounded apex includes the characteristic of when the rounded apex is loaded against a rock formation, the rounded apex fails the rock formation forming a crushed barrier ahead of the rounded apex that shields the rounded apex from a virgin portion of the rock formation while still allowing the rounded apex to penetrate below a surface of the rock formation.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (1)
- Claim 1Independent Claim
A method of degrading a rock formation, comprising: providing a degradation element comprising a substrate bonded to a sintered polycrystalline ceramic comprising a tapering shape and a rounded apex, the rounded apex comprising a curvature with a 0.050 to 0.150 inch radius when viewed from a direction normal to a central axis of the degradation element that intersects the curvature; loading the degradation element along a central axis of the degradation element with 2,000 pounds of load against the rock formation comprising an unconfined compressive strength of 23,000 pounds per square inch, i
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.