CMP pad conditioner, and method for producing the CMP pad conditioner
Abstract
This invention relates to a conditioner for a CMP (Chemical Mechanical Polishing) pad, which is used in a CMP process which is part of the fabrication of a semiconductor device, and more particularly, to a CMP pad conditioner in which the structure of the cutting tips is such that the change in the wear of the polishing pad is not great even when different kinds of slurry are used and when there are changes in pressure of the conditioner, and to a method of manufacturing the same.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A CMP (Chemical Mechanical Polishing) pad conditioner, comprising: a substrate; and a plurality of cutting tips protruding upwards from a surface of the substrate and spaced apart from each other, wherein the cutting tips have a structure in which a top surface of each of the cutting tips is a plane parallel to the surface of the substrate, and wherein the plurality of cutting tips comprises a number of cutting tips such that, under a load applied to the CMP pad conditioner for conditioning, an average pressure applied to each of the cutting tips ranges from 1.55×10 −4 lbf/in 2 to 3.1×10 −2
- Claim 2Depends on #1
The CMP pad conditioner of claim 1 , wherein an upper portion of the cutting tips is formed so that an outer surface defined by connecting an outer circumference of the top surface of the cutting tips to an outer
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (22)
Non-Patent Literature (5)
- Chinese Office Action dated Jul. 1, 2015, issued to Chinese Application No. 201280023632.9.
- International Search Report mailed Jan. 2, 2013, issued in corresponding International Application No. PCT/KR2012/003788.
- Japanese Office Action dated Jul. 29, 2014, issued to the corresponding Japanese Application No. 2014-511292.
- Korean Office Action dated Dec. 9, 2011, issued in corresponding Korean Application No. 10-2011-0046305.
- S.K. Kang et al., "The properties of pad conditioning according to manufacturing methods of CMP pad conditioner", Korea Society for Precision Engineering, Journal of 2005 Fall Conference, pp. 362-365, 2005.