Patents
US 9,278,487 B2#61527036 Most CitedActiveUnited States (USPTO)Utility

Mono-and multi-layer blown films

1Forward Citations (#61527036 Global)
0.1/yrCitation Velocity (#46388013 Global)
0.75Citation PageRank (#61527036 Global)
22Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An extruded air cooled blown film having a) a total thickness of 5 to 500 μm, b) a mono-layer structure or 2 to 9 coextruded layers, c) at least one layer L containing a polymer selected from the group consisting of polypropylene homopolymers, polypropylene random copolymers, hetero-phasic polypropylene block copolymers, or any mixtures thereof, said polymer having a melt flow rate, according to ASTM D-1238, of 0.1 to 10 dg/min at 230° C. and 2.16 kg, said layer L further containing 0.001 to 2%, relative to the weight of the polymer, of a particular nucleating agent, and optionally d) a Modulus according to EN ISO 527 enhanced by at least 10% versus a reference film without the nucleating agent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the manufacture of an extruded air cooled blown film with an industrial blown film line comprising I) admixing a nucleating agent of formula (IA), (IB) or (IC) with a polymer selected from the group consisting of polypropylene homopolymer, polypropylene random copolymer, hetero-phasic polypropylene block copolymer and mixtures thereof in a batch-wise or continuous manner, II) melt extruding the admixture on a single- or twin-screw extruder to achieve homogeneity within the resulting melt at a temperature of at least 20° C. above the melting point of the polymer, III) pressing said

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 3,551,540 AProcess for the continuous production of uniaxially and biaxially oriented films197037
US 4,400,428 ASealable multilayer films198347
CN 1,098,725 ABased on porous stretched article of acrylic resin and preparation method thereof—10
US 5,491,188 APorous stretched article of polypropylene-based resin and process for its preparation199642
JP H08230014 AManufacture of easily tearable propylene-based resin nonoriented film—3
EP 0,765,911 A2Reinforced biodegradable plastics—11
WO 0,004,090 A1Method for reducing tearing in blown polyolefin films—9
EP 1,118,638 A1Flexible syndiotactic polypropylene compositions and molded object—16
US 6,270,911 B1Propylene-based random copolymers and propylene-based resin compositions, films thereof and propylene-based resin laminates200116
US 6,300,415 B1Propylene composition, process for preparing the same, polypropylene composition, and molded articles2001122
US 2002127382 A1Multilayer composite film and use of this film—8
US 2003054161 A1Nonoriented stiff packaging film with superior tear properties—26
US 2003207137 A1Sealable multi-layer opaque film—32
WO 2004/072168 A2Resin compositions—70
WO 2005/026240 A1Polypropylene blown film—8
WO 2005/035598 A1Polypropylene composition for air quenched blown films—24
US 2005203226 A1Beta crystalline polypropylenes—49
US 7,235,191 B2Polypropylene resin compositions200726
US 2007149663 A1Resin compositions—44
US 7,423,088 B2β Crystalline polypropylenes200826
US 2008249269 A1Electret materials—18
WO 2008/122525 A1Electret materials—22

Non-Patent Literature (5)

  • Ajji et al. Polym. Eng. Sci. vol. 44 (2), 2004, pp. 252-260.
  • Bauer et al. Macromolecules vol. 31, 1998, pp. 7651-7658.
  • Behrendt et al., J. Appl. Polym. Sci. vol. 99, 2006, pp. 650-658.
  • Bhattacharya et al., Polymer Processing Society, 19.-23.6. (2005).
  • C. Salis-Soglio et al., CeNS-BIMF Workshop, 2007, pp. 23.