Degradable balls for use in subterranean applications
Abstract
Degradable balls for downhole use may include an incompliant degradable polymer and a compliant filler material, the incompliant degradable polymer having an elastic modulus of about 2 GPa or greater, and the compliant filler material having an elastic modulus of less than about 2 GPa. Such degradable balls may be useful in sealing segments of a wellbore and actuating wellbore tools.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 7.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method comprising: introducing a degradable ball into a wellbore penetrating a subterranean formation, wherein the degradable ball comprises an incompliant degradable polymer and a compliant filler material, the incompliant degradable polymer having an elastic modulus of about 2 GPa or greater, and the compliant filler material having an elastic modulus of less than about 2 GPa; seating the degradable ball in a baffle arranged within the wellbore, and thereby reducing a fluid flow through the baffle and defining an upper segment of the wellbore and a lower segment of the wellbore; treating t
- Claim 2Depends on #1
The method of claim 1 , wherein tr
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (30)
Non-Patent Literature (5)
- International Preliminary Report on Patentability for PCT/US2012/056335 dated Apr. 17, 2014.
- International Search Report and Written Opinion for PCT/US2014/038739 dated Sep. 17, 2014.
- Molnar, K., Factors Affecting the Properties of PLA/CaSO4 Composites: Homogeneity and Interactions, Express Polymer Letters, vol. 3, No. 1, Dec. 2008, pp. 49-61, XP055045125.
- Official Action for Australian Patent Application No. 2010212653 dated Aug. 1, 2013.
- Ultrafine Rubber Particles Raise Thermoplastic's Glass Transition Temperature, Society of Plastics Engineers Plastics Research Online-10.2417/spepro.004492, 2012.