Methods for constructing underground borehole configurations and related solution mining methods
Abstract
Disclosed are methods for solution mining of evaporite minerals, such as trona, comprising drilling an access well and at least two lateral boreholes; injecting a fluid; circulating the fluid through the lateral boreholes with a controlled fluid flow; and collecting a pregnant solution. Also disclosed are methods of solution mining that include injecting an aqueous solution into an underground trona cavity at a temperature sufficient to maintain at least a portion of the solution in the cavity in the Wegscheiderite solid phase region; removing aqueous solution from the cavity; and recovering alkaline values from the removed aqueous solution. Also disclosed are methods of solution mining that include injecting an aqueous solution into an underground trona cavity; removing aqueous solution from the cavity, wherein the temperature of the removed aqueous solution is at about the TWA point temperature; and recovering alkaline values from the removed aqueous solution.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of constructing an underground configuration comprising: a) drilling at least one access well; and b) drilling at least two lateral boreholes, wherein the at least two lateral boreholes are directly communicating with each other and wherein at least one of the lateral boreholes is connected to the at least one access well; wherein construction of said underground configuration allows for and facilitates the management of fluid flow in the lateral boreholes, wherein controlled measurable fluid flow is maintained through the lateral boreholes by the use of components or methods selected
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 11,634,978 B2 | Methods for recovering a mineral from a mineral-bearing deposit | 2023 | 2 |
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- "Directional Drilling," Schlumberger website, as early as Jul. 14, 2002, available at www.glossary.oilfield.slb.com/Display.cfm?Term=directional%20drilling, printed on Jun. 16, 2004, 1 page.
- "Mining Methods," Pangea.Stanford.edu Website, as early as Feb. 24, 2001, available at pangea.stanford.edu/~kurt/tour/kurt-mining-methods.html, printed on Jun. 23, 2004, pp. 1-3.
- "Mining Methods," Pangea.Stanford.edu Website, as early as Feb. 24, 2001, available at pangea.stanford.edu/˜kurt/tour/kurt-mining-methods.html, printed on Jun. 23, 2004, pp. 1-3.
- Day, R., "Solution Mining of Colorado Nahcolite," Wyoming State Geological Survey Information Circular 40, 1998, pp. 121-130.
- Day, R., "White River Nahcolite Solution Mine," Technical Paper, Society for Mining, Metallurgy, and Exploration, Preprint No. 94-210, Feb. 1994, pp. 1-4.