Process for producing a reforming catalyst and the reforming of methane
Abstract
The present invention relates to a process for producing a catalyst for the reforming of hydrocarbons, preferably methane, in the presence of CO 2 , water and/or hydrogen. The production of the catalyst is based on contacting of a hydrotalcite-comprising starting material with a fusible metal salt. The compounds which have been brought into contact with one another are intimately mixed and treated thermally, resulting in the fusible metal salt forming a melt. After molding, the material is subjected to a high-temperature calcination step. The metal salt melt comprises at least one metal selected from the group consisting of K, La, Fe, Co, Ni, Cu and Ce, preferably Ni. The metal salt melt more preferably comprises nickel nitrate hexahydrate. In addition, the invention relates to the use of the catalyst of the invention for the reforming of hydrocarbons, preferably methane, in the presence of CO 2 , water and/or hydrogen at elevated pressures which are greater than 5 bar, preferably greater than 10 bar, particularly preferably greater than 20 bar. The catalyst according to the invention is distinguished from the prior art by particular, preferred physicochemical properties.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 6.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A catalyst, comprising: nickel-magnesium mixed oxide; magnesium spinel; and optionally aluminum oxide hydroxide, wherein the nickel-magnesium mixed oxide has an average crystallite size of ≦100 nm, the magnesium spinel has an average crystallite size of ≦100 nm, a proportion of nickel in the catalyst is in the range of 6-30 mol %, a proportion of magnesium in the catalyst is in the range of 8-38 mol %, a proportion of aluminum in the catalyst is in the range of 50-70 mol % and an intensity of the diffraction reflection of the catalyst at 43.09°2θ is less than or equal to an intensity of the di
- Claim 2Depends on #1
The catalyst according to claim 1 , wherein a BET surface area of the catalyst is in the range of from 10 to 200 m 2 /g.
- Claim 3Independent Claim
The catalyst according to claim
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (20)
Non-Patent Literature (5)
- A. Djaidja et al., "Characterization and activity in dry reforming of methane on NiMg/Al and Ni/MgO catalysts", Catalysis Today, vol. 113, 2006, pp. 194-200.
- Bernard C. Lippens et al., "The Preparation and Properties of Lanthanum-Promoted Nickel-Alumina Catalysts: Structure of the Precipitates", Solid State Ionics, vol. 16, 1985, pp. 275-282.
- C. Gennequin et al., "Use and observation of the hydrotalcite "memory effect" for VOC oxidation", Catalysis Today, vol. 157, 2010, pp. 191-197.
- Carlos Enrique Daza et al., "High stability of Ce-promoted Ni/Mg-Al catalysts derived from hydrotalcites in dry reforming of methane", Fuel, vol. 89, 2010, pp. 592-603.
- Catherine Batiot-Dupeyrat et al., "CO2 reforming of methane over LaNiO3 as precursor material", Catalysis Today, vol. 107, No. 108, 2005, pp. 474-480.