Patents
US 9,252,425 B2#33694682 Most CitedActiveUnited States (USPTO)Utility

Polyacrylonitrile-sulphur composite material

3Forward Citations (#33694682 Global)
0.3/yrCitation Velocity (#25875052 Global)
1.01Citation PageRank (#41000584 Global)
1Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a method for preparing a polyacrylonitrile-sulfur composite material, in which, polyacrylonitrile is converted to cyclized polyacrylonitrile, and the cyclized polyacrylonitrile is reacted with sulfur to form a polyacrylonitrile-sulfur composite material. By a separation of the preparation method into two partial reactions, the reaction conditions are advantageously able to be optimized for the respective reactions and a cathode material is able to be provided for alkali-sulfur cells with improved electrochemical properties. In addition, the invention relates to a polyacrylonitrile-sulfur composite material, a cathode material, an alkali-sulfur cell or an alkali-sulfur battery as well as to an energy store.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: in a first step (a), applying polyacrylonitrile, without adding any sulfur matter to the polyacrylonitrile, to an environment by which the polyacrylonitrile is converted to cyclized polyacrylonitrile; and in a second step (b) that is performed subsequent to performance of the first step (a), applying a mixture, including the cyclized polyacrylonitrile produced by the first step (a) and sulfur, to an environment by which the mixture forms a polyacrylonitrile-sulfur composite material.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein step (a) takes place in an oxygen-containing atmosphere.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein step (a) takes place at a temperature in a range of ≧150° C. to ≦500° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)

Non-Patent Literature (5)

  • International Search Report, PCT International Application No. PCT/EP2012/053855, dated Apr. 26, 2012.
  • Wang J. et al. "Sulfur Composite Cathode Materials for Rechargeable Lithium Batteries," Advanced Functional Materials, vol. 13, No. 6, pp. 487-492, 06-0t-2003.
  • Wang J. et al. "Sulfur Composite Cathode Materials for Rechargeable Lithium Batteries," Advanced Functional Materials, vol. 13, No. 6, pp. 487-492, Jun. 1, 2003.
  • Yu X-G et al. "Lithium Storage in Conductive Sulfur-Containing Polymers," Journal of Eiectroanalytical Chemistry and Interfacialelectro Chemistry, vol. 573, No. 1, pp. 122, 124, Nov. 15, 2004.
  • Yu X-G et al. "Lithium Storage in Conductive Sulfur-Containing Polymers," Journal of Electroanalytical Chemistry and Interfacialelectro Chemistry, vol. 573, No. 1, pp. 122, 124, Nov. 15, 2004.