Abstract

A profiled wire, of NACE grade, made of low-alloy carbon steel intended to be used in the offshore oil exploitation sector is provided. The profiled wire includes the following chemical composition, expressed in percentages by weight of the total mass: 0.75<% C<0.95; 0.30<% Mn<0.85; Cr≦0.4%; V≦0.16%; Si≦1.40% and preferably ≧0.15%; and optionally no more than 0.06% Al, no more than 0.1% Ni and no more than 0.1% Cu, the balance being iron and the inevitable impurities arising from smelting the metal in the liquid state. The steel is obtained, from hot-rolled rod stock cooled down to room temperature, and then having a diameter of about 5 to 30 mm, by subjecting this starting rod firstly to a thermomechanical treatment comprising two successive steps carried out in order, namely an isothermal quench, giving it a homogeneous perlitic microstructure, followed by a mechanical transformation operation carried out cold with an overall degree of work-hardening (or reduction ratio) of between 50 and 80% at most, so as to give the wire its definitive shape, and in that the profiled wire thus obtained is then subjected to a restoration heat treatment of short duration carried out

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A profiled wire of hydrogen-embrittlement-resistant, low-alloy carbon steel for flexible pipelines for the offshore oil and gas operations sector, comprising: a chemical composition, expressed in percentages by weight of the total mass, 0.75<C %<0.95; 0.30<Mn %<0.85; Cr≦0.4%; V≦0.16%; and Si≦1.40% the rest being iron and the inevitable impurities originating from smelting of the metal in the liquid state, and in that, starting from a wire rod, hot-rolled in its austenitic region above 900° C. then cooled to ambient temperature, and then having a diameter of approximately 5 to 30 mm

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • International Search Report Issued Jul. 18, 2011 in PCT/FR11/00167 Filed Mar. 23, 2011.