Patents
US 9,243,107 B2#6500839 Most CitedActiveUnited States (USPTO)Utility

Methods of preparing polyhemiaminals and polyhexahydrotriazines

15Forward Citations (#6500839 Global)
1.5/yrCitation Velocity (#3523502 Global)
1.83Citation PageRank (#16799984 Global)
17Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Polyhexahydrotriazine (PHT) film layers are formed by a process comprising heating a first mixture comprising i) a solvent, ii) paraformaldehyde, and iii) a diamine monomer comprising two primary aromatic amine groups at a temperature of about 20° C. to less than 150° C. This heating step forms a stable polyhemiaminal (PHA) in solution, which can be cast on a surface of a substrate, thereby forming an initial film layer comprising the PHA. The initial film layer is heated at a temperature of 180° C. to about 280° C., thereby converting the PHA film layer to a PHT film layer. Young's moduli of about 8 GPA to about 14 GPA have been observed for the PHT film layers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 15.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method, comprising: forming a reaction mixture comprising a i) solvent, ii) paraformaldehyde, and iii) a monomer comprising two primary aromatic amine groups; and heating the reaction mixture at a temperature of 150° C. to about 280° C., thereby forming a polyhexahydrotriazine (PHT).

  2. Claim 2Independent Claim

    A method, comprising: forming a first mixture comprising a i) solvent, ii) paraformaldehyde, and iii) a monomer comprising two primary aromatic amine groups; heating the first mixture at a temperature of about 20° C. to about 120° C., thereby forming a second mixture comprising a polyhemiaminal (PHA); casting the second mixture on a surface of a substrate, thereby forming an initial film layer disposed on the surface, the initial film layer comprising the PHA and the solvent; and heating the initial film layer at a temperature of 150°

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Chinese Patent Office PCT Search Report, Dec. 29, 2014.
  • Elbert, et al. "Conjugate Addition Reactions Combined with Free-Radical Cross-Linking for the Design of Materials for Tissue Engineering," Biomacromolecules 2001, 2, 430-441; Published on Web Mar. 3, 2001.
  • Ferrar, "Reactions of Formaldehyde With Aromatic Amines," J. Appl. Chem, 14, 1964, 389-399.
  • Geng, et al., "Nanoindentation behavior of ultrathin polymeric films," Polymer 46 (2005) 11768-11772; Available online Oct. 19, 2005.
  • Hiller, et al., "Laser-engravable hexahydrotriazine polymer networks," Mat Res Innovat (2002) 6:179-184.