Abstract
A preparation method of a perfluorinated polymer hollow fiber membrane comprises: evenly mixing a first mixture that is mixed by a perfluorinated polymer, PS, a polymer additive, and a composite pore-forming agent; evenly mixing a second mixture that is mixed by the first mixture and an organic liquid; under 300° C.-350° C., processing the second mixture with a melt to spin by a twin-screw extruder; extruding a hollow fiber by a hollow fiber spinneret; dipping the hollow fiber membrane into deionized water for 48 hours; putting the hollow fiber membrane aired into a concentrated sulfuric acid to process with a sulfonation; washing the hollow fiber membrane by deionized water; and drying the hollow fiber membrane; in such a manner that the hydrophilic perfluorinated polymer hollow fiber membrane is obtained.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A preparation method of a perfluorinated polymer hollow fiber membrane, wherein the preparation method of the perfluorinated polymer hollow fiber membrane uses a membrane formation system, comprising: a perfluorinated polymer, polystyrene (PS), a polymer additive, a composite pore-forming agent, and an organic liquid; wherein, a scope of a mass percent of the perfluorinated polymer is 40 wt %-60 wt %, the scope of the mass percent of the PS is 2 wt %-10 wt %, the scope of the mass percent of the polymer additive is 10 wt %-20 wt %, the scope of the mass percent of the composite pore-forming ag
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗