Nickel bis diazabutadiene precursors, their synthesis, and their use for nickel containing films depositions
Abstract
Disclosed are homoleptic diazabutadiene nickel precursors used for the vapor deposition of nickel-containing films. The precursors have the general formula Ni(R-DAD) 2 , wherein R-DAD stands for substituted 1,4-diazabuta-1,3-diene ligands. The sole presence of the Ni—N bonds was also considered to avoid too high intrusion of other elements, such as carbon, into the nickel-containing films. The flexibility of the Ni—N bond in terms of film deposition also allows using the molecules for nickel, nickel-nitride, nickel-carbonitride, nickel oxide or any other type of nickel-containing films. The nickel-containing film depositions can be carried out by thermal and/or plasma-enhanced CVD, ALD, and pulse CVD or any other type of depositions methods.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of depositing a nickel containing film, the method comprising: introducing at least one nickel bis diazabutadiene precursor into a reactor having at least one substrate disposed therein, the at least one nickel bis diazabutadiene precursor being Ni(nPrN═CH—CH═NnPr) 2 or Ni(iPrN═CH—CH═NiPr) 2 ; and depositing at least part of the nickel bis diazabutadiene precursor onto the at least one substrate to form the nickel containing film.
- Claim 2Depends on #1
The method of claim 1 , wherein the nickel bis diazabutadiene precursor is Ni(nPrN═CH—CH═NnPr) 2 .
- Claim 3Depends on #1
The method of claim 1 , wherein the method is performed at a temperature between about 20° C. and about 600° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,180,234 B2 | Metal organic compounds | 2024 | 0 |
| US 9,991,112 B2 | Method for forming dielectric film and method for fabricating semiconductor device | 2018 | 3 |
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Asplund, M.C. et al., "Time-resolved infrared dynamics of C-F bond activation by a tungsten metal-carbonyl," The Journal of Physical Chemistry B., vol. 110, No. 1, Jan. 1, 2006, pp. 20-24.
- Becht, M. et al., "Nickel thin films grown by MOCVD using Ni(dmg)2 as precursor," Journal de Physique IV, Colloque C5, Journal de Physique II supplement, vol. 5, Jun. 1995, pp. C5-465-C5-472.
- Boo, J.H. et al., "Growth of magnesium oxide thin films using single molecular precursors by metal-organic chemical vapor deposition," Thin Solid Films 341 (1999), 63-67.
- Brissonneau, L. et al., "MOCVD-processed Ni films from nickelocene. Part I: Growth rate and morphology," Chem. Vap. Deposition, 1999, vol. 5, No. 4, pp. 135-142.
- Bruder, H., "3. Diazadien-Metall(O)-Komplexe," Dissertation, Frankfurt Univ., Frankfurt, Germany 1977, 133-216 and English translation.