Patents
US 9,200,710 B2#61569722 Most CitedActiveUnited States (USPTO)Utility

Floating seal

1Forward Citations (#61569722 Global)
0.1/yrCitation Velocity (#47793305 Global)
0.75Citation PageRank (#61569722 Global)
29Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A floating seal comprises C, Si, Mn, Ni, Cr, Mo, V, and B with the remainder being made up of Fe and unavoidable impurities. The contents of the C, Si, Mn, Ni, Cr, Mo, V and B are C: 2.2 to 3.9 wt %, Si: 0.5 to 3.5 wt %, Mn: 0.1 to 2.0 wt %, Ni: 0.5 to 4.3 wt %, Cr: 7.5 to 25.0 wt %, Mo: 0 to 8.0 wt % (excluding 0 %), V: 0 to 6.0 wt % (excluding 0%), and B: 0.02 to 0.4 wt %. The content of Cr in the parent phase is 2.00 to 5.41 wt %. The content of graphite is 0.05 to 0.35% of the surface area. The content of carbon boride is 19 to 40% of the surface area.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A floating seal comprising C, Si, Mn, Ni, Cr, Mo, V, and B with a remainder being made up of Fe and unavoidable impurities, wherein the the floating seal contains C, Si, Mn, Ni, Cr, Mo, V, and B in amounts as follows: C: 2.2 to 3.9 wt % Si: 0.5 to 3.5 wt % Mn: 0.1 to 2.0 wt %; Ni: 0.5 to 4.3 wt %; Cr: 7.5 to 25.0 wt %; Mo: greater than 0 to 8.0 wt %; V: greater than 0 to 6.0 wt %; B: 0.02 to 0.4 wt %; and a content of Cr in a parent phase is 2.00 to 5.41 wt %; a content of graphite is 0.05 to 0.35% of a surface area of the floating seal, and a content of carbon boride is 19 to 40% of the surfa

  2. Claim 2Depends on #1

    The floating seal according to claim 1 , wherein the content of Cr in the parent phase is 2.00 to 3.5 wt %; the content of graphite is 0.05 to 0.30% of the surface area, and the content of carbon boride

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
US 2,662,011 AAbrasion and corrosion resistant white cast iron195316
US 3,588,128 ARotary seal,for oil pumps197114
US 3,897,956 AOil seal member for use in rotary internal combustion engine19756
US 4,505,485 ARotary seal with linear wear resistant treated layer198526
US 4,822,415 AThermal spray iron alloy powder containing molybdenum, copper and boron1989125
US 4,844,483 AFloating seal device198978
US 5,085,716 AHot worked rare earth-iron-carbon magnets199214
US 5,149,249 AShaft seal assembly, especially for high-pressure turbocompressors199225
JP H0790475 AProduction of seal ring for floating seat—15
US 5,525,779 AIntermetallic alloy welding wires and method for fabricating the same199640
JP H1099953 ACentrifugal casting method—8
US 6,045,029 AEarth-boring bit with improved rigid face seal200020
JP 2002234026 ASeal structure of rubber mixing-kneading device—8
US 2002195180 A1Nodular cast iron alloy—14
WO 2005/012585 A1Sintered sliding member and working implement-connecting apparatus—15
US 2005183794 A1Cast iron material, seal material and the production method—5
JP 2005240065 ACast iron material, sealing material and method for manufacturing the sealing material—13
US 6,953,508 B2High strength steel weld having improved resistance to cold cracking and a welding method200522
US 2006159376 A1Sintered sliding member and working implement-connecting apparatus—27
US 2007045966 A1Coatings for metal-metal seal surfaces—33
US 2007187369 A1Hard-facing alloys having improved crack resistance—23
US 2007194537 A1Slide-ring gasket—7
JP 2008221312 ACentrifugal casting device—6
JP 2008221311 AMethod for manufacturing hollow member—4
US 2009045586 A1Method For Producing Rotary and/or Stationary Seal Rings of a Mechanical Face Seal by Means of Laser Hardening—13
US 2010065163 A1Ductile metallic glasses—15
US 2010119872 A1Iron-based hard facing alloys with rare earth additions—5
US 2011162612 A1Iron-chromium alloy with improved compressive yield strength and method of making and use thereof—19
US 8,765,052 B2Abrasion and corrosion resistant alloy and hardfacing/cladding applications20146

Non-Patent Literature (2)

  • The International Search Report for the corresponding international application No. PCT/JP2012/074903, issued on Jul. 24, 2013.
  • The Office Action for the corresponding Korean application No. 10-2014-7011570, issued on Jul. 13, 2015.