US 9,200,342 B2#61319394 Most CitedActiveUnited States (USPTO)Utility

Hot-rolled steel sheet and manufacturing method thereof

1Forward Citations (#61319394 Global)
0.1/yrCitation Velocity (#47782091 Global)
0.75Citation PageRank (#61319394 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A hot-rolled steel sheet according to the present invention is a steel sheet containing a predetermined components, and satisfying O<S/Ca<0.8, N−14/48×Ti≧“0” (zero) %. It is a high-strength hot-rolled steel sheet for a spiral pipe excellent in low-temperature toughness in which a pro-eutectoid ferrite fraction is 3% or more and 20% or less, and the other is a low-temperature transformation phase in a microstructure at a depth of a half thickness of a sheet thickness from a steel sheet surface, a number average crystal grain size of a whole of the microstructure is 2.5 μm or less, an area average grain size is 9 μm or less, a standard deviation of the area average grain size is 2.3 μm or less, and a reflected X-ray intensity ratio {211}/{111} in a direction and in a {111} direction relative to a plane in parallel to the steel sheet surface at the depth of the half thickness of the sheet thickness from the steel sheet surface is 1.1 or more. The steel sheet has both high-toughness and strength of API5L-X80 standard or more.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A hot-rolled steel sheet, comprising by mass %: C=0.02% to 0.06%; Si=0.05% to 0.5%; Mn=1% to 2%; Nb=0.05% to 0.12%; Ti=0.005% to 0.02%; P≦0.03%; S≦0.005%; V≦0.003%; Al=0.005% to 0.1%; N=0.0015% to 0.006%; Ca=0.0005% to 0.003%; V 0.15% (0 (zero) % is not included); Mo≦0.3% (0 (zero) % is not included) N−14/48×Ti≧0 (zero) %; and the remaining portion made up of Fe and inevitable impurity elements, wherein a polygonal ferrite fraction is 3% or more and 20% or less, and the others are a low-temperature transformation phase and pearlite of 1% or less in a microstructure at a depth of a half thickne

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
WO 03,025,241 A1Hot-rolled steel sheet with good ultra low temperature toughness and the method of the same—7
EP 1,462,535 A1Hot-rolled steel strip for high strength electric resistance welding pipe and manufacturing method thereof—22
JP 2004315957 AHigh strength hot rolled steel strip with excellent low-temperature toughness and weldability for resistance welded pipe, and its manufacturing method—40
US 2005183798 A1Hot-rolled steel sheet for high-strength electric-resistance welded pipe having sour-gas resistance and exellent weld toughness, and method for manufacturing the same—17
EP 1,568,792 A1Hot-rolled steel sheet for high-strength electric-resistance welded pipe and method for manufacturing the same—17
JP 2005281838 AHigh strength and high toughness hot rolled steel strip having excellent uniformity of material, and its production method—34
JP 2006274338 AHot rolled steel sheet for sour resistant high strength electric resistance welded pipe having excellent hic resistance and weld zone toughness, and method for producing the same—40
JP 3,846,729 B2極低温衝撃靭性の優れたラインパイプ用熱延鋼板及びその製造方法20065
JP 2008240151 AHigh strength hot rolled steel sheet for line pipe having excellent low-temperature toughness, and its manufacturing method—18
JP 2008248384 AHigh-strength hot-rolled steel plate excellent in low-temperature toughness for spiral pipe and manufacturing method therefor—28
US 7,501,030 B2Hot-rolled steel strip for high strength electric resistance welding pipe and manufacturing method thereof200911
EP 2,116,624 A1High-strength hot-rolled steel plate for line pipes excellent in low-temperature toughness and process for production of the same—11
WO 2009/145328 A1High-strength hot-rolled steel sheet for line pipe excellent in low-temperature toughness and ductile-fracture-stopping performance and process for producing the same—20
JP 2010037567 AThick, high-tension hot-rolled steel sheet excellent in low-temperature toughness, and producing method therefor—14
US 2010059149 A1High strength hot rolled steel plate for spiral line pipe superior in low temperature toughness and method of production of same—6
US 2010084054 A1High strength hot rolled steel products for line-pipes excellent in low temperature touchness and production method of the same—11
US 2011079328 A1High strength hot rolled steel sheet for line pipe use excellent in low temperature toughness and ductile fracture arrest performance and method of production of same—17
US 2011126944 A1Thick-walled high-strength hot rolled steel sheet with excellent low-temperature toughness and method for producing same—13

Non-Patent Literature (5)

  • European Search Report dated Feb. 21, 2014 issued in corresponding EP Application No. 11800943.0.
  • International Preliminary Report on Patentability dated Feb. 21, 2013 issued in corresponding PCT Application No. PCT/JP2011/065014.
  • International Search Report dated Sep. 20, 2011, issued in corresponding PCT Application No. PCT/JP2011/065014.
  • Nippon Steel Technical Report, No. 380, 2004, pp. 70-75, and a partial English translation thereof.
  • Yukito Hagiwara and Shiro Miyamoto, "Fracture Mechanics Approach to Evaluate the Effect of Thickness on Fracture Toughness in Heavy Sectioned Steel" The Iron and Steel, vol. 69 (1983), No. 6, pp. 647-654.