Thin lithium-aluminosilicate glass for three dimensional precision molding
Abstract
A thin lithium-aluminosilicate glass is provided. The glass is suitable for three dimensional precision molding and suitable for toughening, wherein after toughening, the glass has a center tension smaller than 50 Mpa, a surface compressive stress of 600-1200 Mpa, and a bending strength of up to 500 MPa. The glass also has a transition point lower than 550° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 9.
Claims (3 — 3 Independent, 0 Dependent)
- Claim 1Independent Claim
A thin lithium-aluminosilicate glass for three dimensional precision molding, comprising: after toughening, a center tensile stress smaller than 50 MPa, a surface compressive stress of 500-1200 MPa, a bending strength of at least 500 MPa, and a glass transition point lower than 550° C.; and a glass composition, based on the total weight, in weight percentage: SiO 2 58-65 wt. % Li 2 O
- Claim 4Independent Claim
6-5.4 wt. % Na 2 O
- Claim 8Independent Claim
1-9.7
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (2)
- International Search Report dated Jun. 2, 2011 corresponding to International Patent Application No. PCT/CN2011/071157.
- Machine Translation JP 2002-174810 A, Jun. 21, 2002.