Process for producing a highly transparent impact-resistant glass ceramic
Abstract
The process for producing a transparent lithium aluminosilicate glass ceramic plate includes ceramicizing a green glass body of the Li 2 O—Al 2 O—SiO 2 system using a ceramization program, which includes heating it, for the purpose of nucleation, to a temperature of 750° C.±20° C. and maintaining the temperature for 20±15 minutes, further heating the green glass body, for the purpose of ceramization, to a temperature of 900±20° C. and maintaining the to temperature for 20±15 minutes and then cooling to room temperature. The transparent plate has a thermal expansion coefficient (CTE) from −0.15×10 −6 /K to +0.15×10 −6 /K at 30 to 700° C. and a brightness value observed at an angle of 2° of ≧80 for a 4-mm thick plate for transmitted normal light.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a transparent plate, said process comprising the following steps: a) preparing a green glass body comprising glass of a Li 2 O—Al 2 O—SiO 2 system; and b) using a ceramization program, said ceramization program comprising heating the green glass body, for the purpose of nucleation, to a nucleation temperature of 750±20° C. and holding said nucleation temperature for 20±15 minutes, further heating of the green glass body, for the purpose of ceramization to a ceramization temperature of 900±20° C. and holding said ceramization temperature for 20±15 minutes, and cooling t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.