Highly hydrothermal-resistant SCR catalyst and manufacturing method therefor
Abstract
An SCR catalyst including iron-containing β-type zeolite has high NO x reducing performance at a high temperature in the presence of a reducing agent, but does not have the sufficient reducing performance at a low temperature (not higher than 200° C.). A high NO x reduction rate of at least 45% at a temperature not higher than 200° C. is achieved by an SCR catalyst containing iron-containing β-type zeolite having a full width at half maximum (FWHM) on the X-ray crystal diffraction ( 302 ) plane of from 0.28 to 0.34° and a weight loss on heating to 900° C. after hydration treatment of from 15.0 to 18.0% by weight. The SCR catalyst can be manufactured by calcining iron-containing β-type zeolite at 700 to 850° C. under an atmosphere of a water vapor concentration of not more than 5% by volume.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An SCR catalyst comprising iron-containing β-type zeolite having a full width at half maximum (FWHM) on the X-ray crystal diffraction (302) plane of from 0.28 to 0.34° and a weight loss on heating to 900 ° C. after standing for 12 hours or more in a desiccator which has a saturated aqueous solution of ammonium chloride filled in a lower part thereof and has an internal pressure of not more than 15 Torr of from 15.0to 18.0% by weight.
- Claim 2Depends on #1
The SCR catalyst as claimed in claim 1 , wherein a proportion of an isolated iron ion relative to the whole amount of iron contained in the catalyst is from 60 to 90%, and an amount of the isolated iron ion is from 1.0 to 3.0% by weight relative to the catalyst weight.
- Claim 3Depends on #1
The SCR catalyst as claimed in claim 1 , wherein an amount of ion-exchanged iron contained in the ca
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 11,298,692 B2 | Active SCR catalyst | 2022 | 0 |
| US 10,981,089 B2 | Underdrain assembly and method of manufacturing same | 2021 | 0 |
References Cited — Backward Prior Art (22)
Non-Patent Literature (5)
- China Office action in CN 201080038124.9, dated Aug. 29, 2014 along with an english translation thereof.
- Chinese office action in CN201080038124.9, dated Mar. 7, 2014 along with an english translation thereof.
- E.P.O. Office action, mail date is Mar. 4, 2014.
- Extended European Search Report issued with respect to counterpart European Application No. 10811896.9-1213/2471597, dated Jan. 24, 2013.
- Japanese office action in JP 2010-189436, dated Apr. 24, 2014 along with an english translation thereof.