Process for the preparation of expandable vinyl aromatic polymers with a reduced thermal conductivity by polymerization in suspension
Abstract
Process for the preparation of beads of expandable vinyl aromatic polymers by means of polymerization in aqueous suspension, which comprises polymerizing at least one vinyl aromatic monomer in aqueous suspension in the presence of a peroxide initiator system, active at a temperature higher than 800 C, an expanding agent, and in the presence of: —an amide having the general formula R 1 CONHCH 2 —CH 2 NHCOR 2 (I) a flame retardant system comprising a brominated additive with a bromine content higher than 30% by weight.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for preparing a bead of a flame-retardant expandable vinyl aromatic polymer, the process comprising: polymerizing a vinyl aromatic monomer in aqueous suspension, and adding an expanding agent before, during, or after the polymerizing, wherein the process is carried out with a system consisting of water the vinyl aromatic monomer, a peroxide initiator, an amide, a flame-retardant, and optionally the expanding agent; wherein the amide has formula (I): R 1 CONHCH 2 —CH 2 NHCOR 2 (I); wherein R 1 and R 2 are each independently an (iso)alkyl radical CH 3 (CH 2 ) n , a C 6 -C 12 aroma
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (18)
Non-Patent Literature (1)
- International Search Report issued on Oct. 20, 2010 in PCT/IB2010/001983 filed on Aug. 6, 2010.