Method for producing organic light-emitting element
Abstract
Method for manufacturing organic EL element including anode, hole injection layer, buffer layer, light-emitting layer, and cathode, layered on substrate in the stated order, and banks defining a light-emission region, and having excellent light-emission characteristics, due to the hole injection layer having excellent hole injection efficiency, being a tungsten oxide layer including an oxygen vacancy structure, formed under predetermined conditions to have an occupied energy level within a binding energy range from 1.8 eV to 3.6 eV lower than a lowest binding energy of a valence band, and after formation, subjected to atmospheric firing at a temperature within 200° C.-230° C. inclusive for a processing time of 15-45 minutes inclusive to have increased film density and improved dissolution resistance against an etching solution, a cleaning liquid, etc., used in a bank forming process.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for manufacturing an organic light-emitting element, the method comprising: forming a tungsten oxide layer on a base layer including an anode, the tungsten oxide layer containing tungsten oxide and having a first film density; firing the tungsten oxide layer to obtain a fired tungsten oxide layer, the fired tungsten oxide layer having a second film density higher than the first film density; forming a film of barrier wall material on the fired tungsten oxide layer; forming barrier walls by patterning the film of barrier wall material in a predetermined pattern by using an etching solu
- Claim 2Depends on #1
The method of claim 1 , wherein i
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (33)
Non-Patent Literature (5)
- Hiromi Watanabe et al., "Structure and Physical Property Evaluation of MoOX Thin-Film in Reactive Sputtering Method, and MoOX/alpha-NPD Boundary Analysis", (Nov. 20, 2008). Along with a partial English language translation.
- Hiromi Watanabe et al., "Structure and Physical Property Evaluation of MoOX Thin-Film in Reactive Sputtering Method, and MoOX/α-NPD Boundary Analysis", (Nov. 20, 2008). Along with a partial English language translation.
- Hyunbok Lee et al., "The origin of the hole injection improvements at indium tin oxide/molybdenum trioxide/N,N′-bis (1-naphthyl)-N,N′-diphenyl-1,1′-biphenyl-4,4′-diamine interface", Applied Physics Letters 93, 043308 (2008).
- Hyunbok Lee et al., "The origin of the hole injection improvements at indium tin oxide/molybdenum trioxide/N,N'-bis (1-naphthyl)-N,N'-diphenyl-1,1'-biphenyl-4,4'-diamine interface", Applied Physics Letters 93, 043308 (2008).
- I. N. Yakovkin et al., "Driving force for the WO3(001) surface relaxation", Surface Science 601, pp. 1481-1488 (2007).