Abstract
The invention relates a heat-treated poly(metaphenylene isophthalamide) polymer fiber having a crystalline structure as represented by a carbonyl stretch peak at a wavelength of 1,650 cm−1 in a Raman spectra response which before coloration with a dye, shrinks linearly 0.4 percent or less when exposed to 285 degrees Centigrade for 30 minutes; and which after contact with an aqueous red dye solution for 1 hour at 120 degrees Centigrade, has an “L” value coloration of at least 40 units lower than the “L” value of the fiber before coloration.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A poly(metaphenylene isophthalamide) polymer fiber having a crystalline structure as represented by a carbonyl stretch peak at a wavelength of 1,650 cm −1 in a Raman spectra response; said fiber, before coloration with a dye, shrinks linearly 0.4 percent or less when exposed to 285 degrees Centigrade for 30 minutes; and said fiber, after contact with an aqueous red dye solution for 1 hour at 120 degrees Centigrade, has an “L” value coloration of at least 40 units lower than the “L” value of the fiber before coloration.
- Claim 2Depends on #1
The polymer fiber of claim 1 , wherein the “L” value of the fiber after coloration is 45 or less.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.