Processes for production of silicon ingot, silicon wafer and epitaxial wafer, and silicon ingot
Abstract
A process for production of a silicon ingot, by which a silicon ingot exhibiting a low resistivity even in the top portion can be produced. The process for the production of a silicon ingot includes withdrawing a silicon seed crystal from a silicon melt to grow a silicon single crystal, with the silicon seed crystal and the silicon melt containing dopants of the same kind. The process includes the dipping step of dipping a silicon seed crystal containing a dopant in a specific concentration in a silicon melt in such a manner that the temperature difference between both falls within the range of 50 to 97K, and the growing step of growing a silicon single crystal withdrawn after the dipping to form a silicon ingot, the growing step being conducted by using a single crystal puller provided with a thermal shield plate for shielding against radiant heat emitted from the silicon melt and controlling the distance between the thermal shield plate and the silicon melt within a specific range.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 0.
Claims (6)
- Claim 1Independent Claim
A process for manufacturing a silicon ingot, comprising: dipping a seed crystal in a melt in a crucible in a hot zone, wherein: the seed crystal and the melt containing dopants of the same kind, a concentration of the dopant contained in the seed crystal is: 2.0×10 19 to 4.0×10 19 atoms/cm 3 in a case of arsenic; 5.0×10 19 to 7.0×10 19 atoms/cm 3 in a case of phosphorous; and 5.0×10 19 to 7.0×10 19 atoms/cm 3 of phosphorous and 4.0×10 19 to 8.0×10 19 atoms/cm 3 of germanium in a case of a combination of phosphorous and germanium, the temperature difference between the seed crystal and the melt, when dipping the seed crystal in the melt, is 50 to 97 K; and growing the silicon single crystal pulled after the dipping obtain the silicon ingot, wherein the growing comprises using a single crystal puller provided with a thermal shield plate for shielding the silicon ingot against radiant heat from the melt; wherein a distance between the thermal shield plate and a surface of the melt is 20 to 30 mm at the beginning of growing a straight body portion of the silicon ingot, in the growing, a distance between the thermal shield plate and the surface of the melt is 6 to 15 mm in growing the straight body portion from a position of 200 mm away from a boundary between a shoulder portion and the straight body portion in a direction opposite to a pulling direction of the silicon ingot, in the growing, a diameter of the produced silicon ingot is 200 mm; and a length of a region of the produced silicon ingot having resistivity of no greater than 1.6 mΩcm is no less than 200 mm in a longitudinal direction in a case of arsenic; a length of a region of the produced silicon ingot having resistivity of no greater than 0.8 mΩcm is no less than 100 mm in a longitudinal direction in a case of phosphorous; a length of a region of the produced silicon ingot having resistivity of no greater than 0.8 mΩcm is no less than 50 mm in a longitudinal direction in a case of a combination of phosphorous and germanium.
- Claim 2Depends on #1
A silicon ingot that is produced by the process for manufacturing a silicon ingot according to claim 1 and satisfies any one of the following conditions A to C: Condition A: the dopant is arsenic and resistivity of a region in the silicon ingot of 5 to 15% solidification ratio is 1.6 to 2.0 mΩcm; Condition B: the dopant is phosphorous and resistivity of a region in the silicon ingot of 5 to 15% solidification ratio is 0.95 to 1.1 mΩcm; and Condition C: the dopant is a combination of phosphorous and germanium and resistivity of a region in the silicon ingot of 5 to 15% solidification ratio is 1.0 to 1.2 mΩcm.
- Claim 3Depends on #2
The silicon ingot according to claim 2 that further satisfies any one of the following conditions D to F: Condition D: the dopant is arsenic and resistivity of a region in the silicon ingot of 80 to 90% solidification ratio is 1.3 to 1.6 mΩcm; Condition E: the dopant is phosphorous and resistivity of a region in the silicon ingot of 80 to 90% solidification ratio is 0.70 to 0.80 mΩcm; and Condition F: the dopant is a combination of phosphorous and germanium and resistivity of a region in the silicon ingot of 80 to 90% solidification ratio is 0.70 to 0.90 mΩcm.
- Claim 4Depends on #1
The process according to claim 1 , further comprising obtaining a silicon wafer by slicing the silicon ingot.
- Claim 5Depends on #4
A The process according to claim 4 , further comprising obtaining an epitaxial wafer by forming an epitaxial layer on a surface of the silicon wafer.
- Claim 6Independent Claim
A silicon ingot, wherein the silicon ingot is manufactured by the following process: dipping a seed crystal in a melt in a crucible in a hot zone, wherein: the seed crystal and the melt each contain an arsenic dopant, a concentration of the arsenic dopant contained in the seed crystal is: 2.0×10 19 to 4.0×10 19 atoms/cm 3
Technical Overview & Description
TECHNICAL FIELD The present invention relates to processes for production of a silicon ingot, a silicon wafer and an epitaxial wafer, and a silicon ingot produced by the process. BACKGROUND ART In recent years, small-sized devices such as mobile phones are widely used. There is a strong demand for long-lasting power with portable usage of such small-sized devices, and research is being conducted for increasing capacity of a battery used in the small-sized devices and reducing power consumption of the small-sized devices. In order to reduce the power consumption of the small-sized devices, reduction in power consumption of semiconductor devices installed in the small-sized devices is required. For example, a low-voltage power MOSFET (Metal Oxide Semiconductor Field Effect Transistor), used as a power device for the small-sized devices, has a constant internal resistance when the power is on, so that the low-voltage power MOSFET itself consumes electricity according to power current flowing therethrough. Therefore, by reducing the internal resistance in the low-voltage power MOSFET when the power is on, power consumption of the small-sized devices can be reduced. Given this, a low-resistivity N-type single crystal is strongly demanded for reducing the resistance when the low-voltage MOSFET is turned on. A low-resistivity N-type single crystal can be obtained generally by preparing a highly-doped single crystal with an N-type dopant such as arsenic or phosphorous. However, when an ingot is pulled by the Czochralski method by doping a high concentration of an N-type dopant, the degree of solidification point depression is extremely high due to a large amount of dopant, and constitutional supercooling may be caused. When the degree of such constitutional supercooling is extreme, a growth different from that of a silicon growth face may be initiated on a crystal growth interface, which leads to an abnormal growth (cell growth). Such an abnormal gro
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (17)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (4)
- Japan Office action, mail date is Jul. 30, 2013.
- Low On-Resistance MOSFETs Enhance SMPS, EE product news, Oct. 8, 2008.
- U.S. Appl. No. 13/055,990 to Yasuhito Narushima et al., filed Jan. 26, 2011.
- U.S. Appl. No. 13/056,017 to Yasuhito Narushima et al., filed Jan. 26, 2011.