Abstract

A non-flammable quasi-solid electrolyte and a rechargeable non-lithium alkali metal cell containing this electrolyte. The electrolyte comprises an alkali metal salt dissolved in an organic liquid solvent with a concentration higher than 2.5 M (preferably >3.5 M) or a molecular ratio greater than 0.2 (preferably >0.3), wherein the alkali metal is selected from Na, K, a combination of Na and K, or a combination of Na and/or K with Li. The alkali metal salt concentration is sufficiently high so that the electrolyte exhibits a vapor pressure <0.01 kPa when measured at 20° C., a vapor pressure <60% of the vapor pressure of thet organic solvent when measured alone, a flash point at least 20 degrees Celsius higher than a flash point of the organic liquid solvent when measured alone, a flash point higher than 150° C., or no detectable flash point.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 16.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A non-flammable quasi-solid electrolyte for use in a rechargeable alkali metal cell, said electrolyte comprising an alkali metal salt dissolved in an organic liquid solvent with a concentration higher than 2.5 M or said alkali metal salt having a molecular ratio greater than 0.2, wherein said alkali metal is selected from sodium (Na), potassium (K), a combination of Na and K, or a combination of Na and/or K with lithium (Li) and said alkali metal does not include lithium alone.

  2. Claim 2Depends on #1

    The non-flammable quasi-solid electrolyte of claim 1 , wherein said alkali metal salt concentration is sufficiently high so that said electrolyte exhibits a vapor pressure less than 0.01 kPa when measured at 20° C., a vapor pressure less than 60% of the vapor pressure of said first organic solvent when measured alone, a flash point at least 20 degr

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 16 total)

PatentTitleYearCitations
US 11,901,562 B2Bipolar electrodes containing flame-resistant quasi-solid or solid-state electrolyte, bipolar lithium batteries, and manufacturing method20240
CN 107,170,961 AThe preparation method and application of carbon-nitrogen doped ternary metal oxide—9
US 12,308,387 B2Phosphazene compound-based electrolyte compositions, quasi-solid and solid-state electrolytes, and lithium batteries20250
US 11,949,063 B2Flame-resistant quasi-solid hybrid electrolyte for safe anode-less lithium batteries and production method20240
CN 110,354,631 BPreparation method and application of ionic liquid-activated carbon composite viscose20210
US 11,949,109 B2Flame-resistant electrodes lithium containing quasi-solid or solid-state electrolytes and manufacturing method20240
CN 111,204,728 BPreparation method of ultrathin two-dimensional vanadium phosphorus oxygen composite metal oxide nanosheet20210
CN 110,707,359 AElectrolyte for high-voltage lithium ion battery—1
US 11,830,976 B2Flame-resistant electrolyte compositions, quasi-solid and solid-state electrolytes, and lithium batteries20230
CN 110,354,631 AA kind of preparation method and applications of the compound viscose of ionic liquid-active carbon—2
US 11,881,580 B2Flame-resistant bipolar electrodes, bipolar lithium batteries, and manufacturing method20240
US 11,888,119 B2Method of producing flame-resistant quasi-solid electrolytes and lithium batteries containing same20240
CN 111,204,728 APreparation method of ultrathin two-dimensional vanadium phosphorus oxygen composite metal oxide nanosheet—3
CN 109,888,193 AA kind of raising sodium metal negative electrode electro-deposition and dissolve out reversible method—7
US 12,142,729 B2Quasi-solid and solid-state electrolyte for lithium-ion and lithium metal batteries and manufacturing method20240

Non-Patent Literature (3)

  • J. F. Whitacre, "Na4Mn9O18 as a positive electrode material for an aqueous electrolyte sodium-ion energy storage device," Electrochemistry Commun. 12 (2010) 463-466.
  • U.S. Appl. No. 10/858,814 , "Process for producing nano-scaled graphene plates", B.Jang, filed Jun. 3, 2004, now abandoned.
  • Zhuo, X.Y. Wang, A.P. Tang, Z.M. Liu, S. Gamboa, P.J. Sebastian, Journal of Power Sources 160 (2006) 698.