Patents
US 9,059,250 B2#27291458 Most CitedActiveUnited States (USPTO)Utility

Lateral-dimension-reducing metallic hard mask etch

4Forward Citations (#27291458 Global)
0.4/yrCitation Velocity (#22227600 Global)
1.05Citation PageRank (#38944613 Global)
21Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A combination of gases including at least a fluorocarbon gas, oxygen, and an inert sputter gas is employed to etch at least one opening into an organic photoresist. The amount of oxygen is controlled to a level that limits conversion of a metallic nitride material in an underlying hard mask layer to a metal oxide, and causes organic polymers generated from the organic photoresist to cover peripheral regions of each opening formed in the organic photoresist. The hard mask layer is etched with a taper by the oxygen-limited fluorine-based etch chemistry provided by the combination of gases. The taper angle can be controlled such that a shrink ratio of the lateral dimension by the etch can exceed 2.0.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a patterned structure comprising: forming a stack comprising, from bottom to top, at least one underlying material layer comprising at least one dielectric material layer and a dielectric hard mask layer, a metallic hard mask layer, and a photoresist layer; patterning said photoresist layer with a pattern comprising at least one opening therein; transferring said pattern into said metallic hard mask layer in an etch process employing a combination of gases, said combination of gases comprising at least one fluorocarbon gas, oxygen, and at least one inert sputter gas, wherei

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 4,144,119 AEtchant and process197939
US 4,675,073 ATin etch process198745
US 5,851,302 AMethod for dry etching sidewall polymer199828
US 5,925,577 AMethod for forming via contact hole in a semiconductor device199936
US 5,939,748 AStorage capacitor having a refractory metal storage electrode and method of forming the same19999
US 5,968,711 AMethod of dry etching A1Cu using SiN hard mask199925
US 5,982,035 AHigh integrity borderless vias with protective sidewall spacer199933
US 6,057,081 AProcess for manufacturing semiconductor integrated circuit device200049
US 6,100,183 AMethod for fabricating a via200029
US 6,232,223 B1High integrity borderless vias with protective sidewall spacer200112
US 6,261,934 B1Dry etch process for small-geometry metal gates over thin gate dielectric200136
US 6,387,798 B1Method of etching trenches for metallization of integrated circuit devices with a narrower width than the design mask profile200263
US 6,451,673 B1Carrier gas modification for preservation of mask layer during plasma etching200219
US 6,531,404 B1Method of etching titanium nitride200356
US 7,157,375 B2Methods of downstream microwave photoresist removal and via clean, particularly following Stop-On TiN etching20071
US 7,276,450 B2Etching processes using C4F8 for silicon dioxide and CF4 for titanium nitride20077
US 7,354,867 B2Etch process for improving yield of dielectric contacts on nickel silicides20081
US 7,553,772 B1Process and apparatus for simultaneous light and radical surface treatment of integrated circuit structure200914
US 7,638,430 B2Method of forming contact plug of semiconductor device20093
US 2010295147 A1Isolation structure and formation method thereof—8
US 7,863,124 B2Residue free patterned layer formation method applicable to CMOS structures20112