Method of forming a VDF oligomer or co-oligomer film on a substrate and an electrical device comprising the VDF oligomer or co-oligomer film on the substrate
Abstract
A method of forming a vinylidene fluoride (VDF) oligomer or co-oligomer film on a substrate is disclosed. The method comprises forming a VDF oligomer or co-oligomer precursor solution; depositing the VDF oligomer or co-oligomer precursor solution onto the substrate to form a preliminary VDF oligomer or co-oligomer film on the substrate; and applying uniaxial pressure on the preliminary VDF oligomer or co-oligomer film and the substrate at an elevated temperature to form the VDF oligomer or co-oligomer film on the substrate. The substrate may comprise a metal surface which may be used as a bottom electrode and a top electrode may be deposited on the VDF oligomer or co-oligomer film. The VDF oligomer or co-oligomer film, the bottom electrode on the substrate and the top electrode on the VDF oligomer or co-oligomer film form an electrical device.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming a VDF oligomer or co-oligomer film on a substrate, the method comprising: forming a VDF oligomer or co-oligomer precursor solution; depositing the VDF oligomer or co-oligomer precursor solution onto the substrate to form a preliminary VDF oligomer or co-oligomer film on the substrate; and applying uniaxial pressure on the preliminary VDF oligomer or co-oligomer film and the substrate at an elevated temperature in the range of 80° C.-135° C. to form the VDF oligomer or co-oligomer film on the substrate.
- Claim 2Depends on #1
A method as claimed in claim 1 , wherein prior to applying uniaxial pressure on the preliminary VDF oligomer or co-oligomer film and the substrate at an elevated temperature, the preliminary VDF oligomer or co-oligomer film and the substrate are annealed at a temperature between 100° C.-150° C. for crys
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (8)
Non-Patent Literature (4)
- PCT International Preliminary Report on Patentability (Chapter II of the Patent Cooperation Treaty) for PCT Counterpart Application No. PCT/SG2009/000494, 4 pgs., (Apr. 24, 2012).
- PCT International Search Report for PCT Counterpart Application No. PCT/SG2009/000494 containing Communication relating to the Results of the International Search Report, 3 pgs., (Feb. 12, 2010).
- PCT Written Opinion of the International Preliminary Examining Authority for PCT Counterpart Application No. PCT/SG2009/000494, 4 pgs., (Dec. 16, 2010).
- PCT Written Opinion of the International Searching Authority for PCT Counterpart Application No. PCT/SG2009/000494, 5 pgs., (Feb. 12, 2010).