Patents
US 9,051,641 B2#22194962 Most CitedActiveUnited States (USPTO)Utility

Cobalt deposition on barrier surfaces

5Forward Citations (#22194962 Global)
0.5/yrCitation Velocity (#18111831 Global)
1.23Citation PageRank (#30990014 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the invention provide processes for depositing a cobalt layer on a barrier layer and subsequently depositing a conductive material, such as copper or a copper alloy, thereon. In one embodiment, a method for depositing materials on a substrate surface is provided which includes forming a barrier layer on a substrate, exposing the substrate to dicobalt hexacarbonyl butylacetylene (CCTBA) and hydrogen to form a cobalt layer on the barrier layer during a vapor deposition process (e.g., CVD or ALD), and depositing a conductive material over the cobalt layer. In some examples, the barrier layer and/or the cobalt layer may be exposed to a gas or a reagent during a treatment process, such as a thermal process, an in situ plasma process, or a remote plasma process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for depositing materials on a substrate surface, comprising: forming a barrier layer on a substrate, wherein the barrier layer comprises a metallic layer, a metal nitride layer, or combinations thereof; exposing the substrate to dicobalt hexacarbonyl butylacetylene (CCTBA) and hydrogen to form a cobalt layer on the barrier layer during a vapor deposition process; and depositing a conductive material over the cobalt layer, wherein the cobalt layer is metallic cobalt, cobalt boride, cobalt phosphide, or combinations thereof.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising exposing the barrier layer or the cobalt layer to a plasma during a treatment process, wherein the plasma is formed from nitrogen (N 2 ), ammonia (NH 3 ), hydrogen (H 2 ), or combinations thereof.

  3. Claim 3Depends on #2

    The method of claim 2 ,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,058,430 AMethod for producing compound thin films19771,251
JP S5898917 AAtomic layer epitaxial device—25
US 4,389,973 AApparatus for performing growth of compound thin films1983653
US 4,413,022 AMethod for performing growth of compound thin films1983555
US 4,415,275 ASwirl mixing device1983115
US 4,486,487 ACombination film, in particular for thin film electroluminescent structures1984179
US 4,500,409 AMagnetron sputter coating source for both magnetic and non magnetic target materials198572
JP S61174725 AThin film forming apparatus—13
US 4,761,269 AApparatus for depositing material on a substrate1988366
JP S6428921 APlasma treatment device—13
US 4,814,294 AMethod of growing cobalt silicide films by chemical vapor deposition198951
US 4,824,544 ALarge area cathode lift-off sputter deposition device1989138
US 4,834,831 AMethod for growing single crystal thin films of element semiconductor1989255
US 4,951,601 AMulti-chamber integrated process system1990968
JP H02246161 AThin-film transistor—23
US 4,975,252 ASemiconductor crystal growth apparatus1990127
JP H02298263 ASputtering device—8
US 4,993,357 AApparatus for atomic layer epitaxial growth1991258
JP H03140487 AElectrochemical reactor—5
US 5,027,746 AEpitaxial reactor having a wall which is protected from deposits1991159
JP H03240944 AMethod and device for focusing target sputtering for forming thin aluminum film—15
US 5,096,364 AWafer arm handler mechanism199259
US 5,122,923 AThin-film capacitors and process for manufacturing the same1992164
JP H04291916 AMethod and apparatus for vapor growth—34
US 5,173,327 ALPCVD process for depositing titanium films for semiconductor devices1992135