Pasted zinc electrode for rechargeable nickel-zinc batteries
Abstract
Active material for a negative electrode of a rechargeable zinc alkaline electrochemical cell is made with zinc metal particles coated with tin and/or lead. The zinc particles may be coated by adding lead and tin salts to a slurry containing zinc particles, a thickening agent and water. The remaining zinc electrode constituents such as zinc oxide (ZnO), bismuth oxide (Bi 2 O 3 ), a dispersing agent, and a binding agent such as Teflon are then added. The resulting slurry/paste has a stable viscosity and is easy to work with during manufacture of the zinc electrode. Further, the zinc electrode is much less prone to gassing when cobalt is present in the electrolyte. Cells manufactured from electrodes produced in accordance with this invention exhibit much less hydrogen gassing, by as much as 60-80%, than conventional cells. The cycle life and shelf life of the cells is also enhanced, as the zinc conductive matrix remains intact and shelf discharge is reduced.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 0.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of making a zinc negative electrode, the method comprising: (a) forming a coating consisting essentially of tin on zinc alloy particles; (b) forming a paste comprising the coated zinc alloy particles, zinc oxide, bismuth oxide, and a binding agent; and (c) incorporating the paste into a zinc electrode, wherein the tin comprises less than about 1% by weight of the paste and, wherein the zinc alloy particles comprise an alloy of zinc with an alloying element selected from the group consisting of bismuth, indium, and combinations thereof, and wherein the zinc alloy particles are less tha
- Claim 2Depends on #1
The method of claim 1 , wherein the coating operation (a) comprises: contacting the zinc alloy particles with a solution comprising at least one soluble tin salt.
- Claim 3Independent Claim
The method
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (38)
Non-Patent Literature (5)
- Chinese Office Action dated Jan. 16, 2015 in CN Application No. 201080022093.8.
- Chinese Office Action dated Jun. 10, 2014 in CN Application No. 201080022093.8.
- Chinese Office Action dated Oct. 10, 2013 in CN Application No. 201080022093.8.
- EP Examination Report dated Feb. 22, 2013 in EP Application No. 10724181.2.
- EP Examination Report dated Jul. 23, 2013 in EP Application No. 10724181.2.