Ni-based superalloy, and turbine rotor and stator blades for gas turbine using the same
Abstract
An object of the present invention is to provide a Ni-based superalloy, especially for a conventional casting, having a good balance among high temperature strength, corrosion resistance and oxidation resistance, as compared to a conventional material. The Ni-based superalloy comprises Cr, Co, Al, Ti, Ta, W, Mo, Nb, C, B, and inevitable impurities, the balance being Ni, the Ni-based superalloy having a superalloy composition comprising, by mass, 13.1 to 16.0% Cr, 11.1 to 20.0% Co, 2.30 to 3.30% Al, 4.55 to 6.00% Ti, 2.50 to 3.50% Ta, 4.00 to 5.50% W, 0.10 to 1.20% Mo, 0.10 to 0.90% Nb, 0.05 to 0.20% C, and 0.005 to 0.02% B.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A Ni-based superalloy comprising Cr, Co, Al, Ti, Ta, W, Mo, Nb, Hf, C, B, Re, Zr, O, N, and inevitable impurities, the balance being Ni, the Ni-based superalloy having a superalloy composition comprising, by mass, 13.1 to 16.0% Cr, 13.1 to 18.0% Co, 2.30 to 3.30% Al, 4.55 to 6.00% Ti, 2.50 to 3.50% Ta, 4.00 to 4.90% W, 0.10 to 1.20% Mo, 0.10 to 0.90% Nb, 0.01 to 0.04% Hf, 0.05 to 0.20% C, 0.005 to 0.02% B, 0.003 to 0.50% Re, 0.01 to 0.05% Zr, 0.001 to 0.005% O and 0.001 to 0.005% N.
- Claim 2Depends on #1
The Ni-based superalloy according to claim 1 , wherein the Ni-based superalloy has a superalloy composition comprising, by mass, 0.003 to 0.10% Re, and 0.01 to 0.03% Zr.
- Claim 3Depends on #2
The Ni-based superalloy according to claim 2 , wherein the Ni-based superalloy has a superalloy composition comprising, by mass, 13.1 to 14.3% Cr, 2.60 to 3.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (28)
Non-Patent Literature (4)
- EP Notice of Opposition of Appln. No. 11195397.2 dated Oct. 4, 2013 with partial English translation.
- EP Search Report dated of Appln. No. 11195397.2 dated Apr. 5, 2012 in English.
- JP Office Action of Appln. No. 2010-293142 dated Mar. 12, 2013.
- Office Action from State Intellectual Property Office of the People's Republic of China (SIPO) of Appln. No. 201110442776.5 dated Sep. 11, 2013 with partial English translation.