Low-density polyurethane shoe soles or sole parts with high rebound resilience and low compression set
Abstract
A process for producing a polyurethane shoe sole having an article density of 100 to 350 g/L and being made from an organic polyisocyanate, a polyol, a blowing agent consisting of water, and optionally a crosslinking and/or chain-extending agent, a catalyst, and other auxiliaries and/or additives. First, polyisocyanate, polyol and any crosslinking and/or chain-extending agent are mixed and reacted at a temperature of 110° C. to 180° C. to give a prepolymer having polyisocyanate groups. Second, the isocyanate-terminated prepolymer obtained and any remaining polyisocyanate are mixed with any remaining polyol, blowing agent comprising water, and any remaining crosslinking and/or chain-extending agent and also any catalyst and other auxiliaries and/or additives are introduced into a mold and allowed to fully react to give a polyurethane shoe sole.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a polyurethane shoe sole having an article density of 100 to 350 g/L, in which components comprising the following are mixed and/or reacted: a) an organic polyisocyanate, b) a polyol, c) a blowing agent comprising water, and optionally d) a crosslinking and/or chain-extending agent, e) a catalyst, and f) at least one auxiliary and/or additive, the process comprising (1) mixing and reacting at least part of polyisocyanate (a), at least part of polyol (b) and at least part of crosslinking and/or chain-extending agent (d) if present, at a temperature of 130° C. to 180° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗