Patents
US 9,023,306 B2#41099000 Most CitedActiveUnited States (USPTO)Utility

Ultratough single crystal boron-doped diamond

2Forward Citations (#41099000 Global)
0.2/yrCitation Velocity (#35669089 Global)
0.99Citation PageRank (#42500571 Global)
21Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a single crystal boron doped CVD diamond that has a toughness of at least about 22 MPa m 1/2 . The invention further relates to a method of manufacturing single crystal boron doped CVD diamond. The growth rate of the diamond can be from about 20-100 μm/h.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for growing single-crystal boron doped diamond of high toughness comprising: i) placing a seed diamond in a heat sink holder made of a material that has a high melting point and high thermal conductivity to minimize temperature gradients across the growth surface of the diamond; ii) controlling the temperature of a growth surface of the diamond such that the temperature of the growing diamond crystals is in the range of 1100-1300° C.; and iii) growing single-crystal diamond by microwave plasma chemical vapor deposition on the growth surface of a diamond in a deposition chamber compris

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
EP 0,390,209 A2Diamond light-emitting device—31
EP 0,390,209 A3Diamond light-emitting device—9
US 5,541,423 AMonocrystalline diamond semiconductor device and several electronic components employing same199658
US 5,981,057 ADiamond199957
US 6,322,891 B1Thermally-diffused boron diamond and its production20017
US 6,858,078 B2Apparatus and method for diamond production200527
US 2005066884 A1Method of growing a single crystal diamond—6
US 2005109266 A1Arc jet microwave plasma method of growing single crystal diamond—6
US 2005139150 A1Diamond single crystal composite substrate and method for manufacturing the same—4
US 2006065187 A1Ultratough CVD single crystal diamond and three dimensional growth thereof—25
US 7,115,241 B2Ultrahard diamonds and method of making thereof200610
WO 2006/127611 A2Colorless single-crystal cvd diamond at rapid growth rate—13
US 7,157,067 B2Tough diamonds and method of making thereof200714
US 7,160,617 B2Boron doped diamond200729
US 2007051300 A1Synthesis of large homoepitaxial monocrystalline diamond—12
US 2007077192 A1Tough diamonds and method of making thereof—7
US 7,201,886 B2Single crystal diamond tool20077
WO 2007/081492 A2High growth rate methods of producing high-quality diamonds—24
US 2007196263 A1Colorless single-crystal CVD diamond at rapid growth rate—23
US 2008003447 A1Materials and methods for the manufacture of large crystal diamonds—25
US 7,883,684 B2Colorless single-crystal CVD diamond at rapid growth rate201110

Non-Patent Literature (5)

  • Anderson et al., "The effect of carbon and nitrogen implantation on the abrasion resistance of type IIa(110) diamond", Nucl. Methods Phys. Res. B 80-81, 1451 (1993).
  • Anstis et al., "Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack Measurements", J. Am. Ceram. Soc. 64, 533 (1981).
  • Anthony et al., "Stresses generated by inhomogeneous distributions on inclusions in diamonds", Diam. Rel. Mater. 6, 120 (1997).
  • Arima et al., "Effects of vicinal angles from (0 0 1) surface on the Boron-doping features of high-quality homoepitaxial diamond films grown by the high-power microwave plasma chemical-vapor-deposition method", J. Crys. Growth, 309, pp. 145-152 (2007).
  • Brazhkin et al., "From our readers: What does 'harder than diamond' mean?" Nature Materials, 3(9), 576 (2004).