Low carbon-dioxide additive compositions and warm-mix asphalt binder and mixture production method using the additive
Abstract
Provided are a low carbon additive for a warm-mix asphalt (WMA) mixture, in which vegetable wax based on modified palm wax is mixed into polyethylene wax so as to be able to promote high-temperature physical properties of the WMA mixture as well as solve problems on low-temperature physical properties of the WMA mixture, warm-mix asphalt produced using the same, and a method of producing the WMA mixture using the using the warm-mix asphalt. The low carbon additive contains polyethylene wax and vegetable wax at a weight ratio of 20:1 to 1:2. The modified palm wax employs palm wax that melt-reacts with sodium hydroxide (NaOH) and stearic acid (CH 3 (CH 2 ) 16 COOH). This low carbon additive enables the WMA mixture to be efficiently produced, and thus makes it possible to reduce heating energy required when the WMA mixture is produced. Thereby, it is possible to remarkably reduce the emission of carbon dioxide that is a principal factor of global warming.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A low carbon additive for a warm-mix asphalt mixture, comprising polyethylene wax and vegetable wax, wherein the polyethylene wax and the vegetable wax are contained at a weight ratio of 20:1 to 1:2, and the vegetable wax is a modified palm wax having a melting point of 90° C. to 110° C., and the modified palm wax is a melt reaction product of a hydrogenating palm oil extracted from a coconut, with sodium hydroxide (NaOH) and stearic acid (CH 3 (CH 2 ) 16 COOH, wherein the palm wax and the sodium hydroxide used for the modified palm wax have a weight ratio of 100:3.5 to 100:4.0, and the palm w
- Claim 2Depends on #1
The low carbon additive according to claim 1 , wherein the polyethylene wax has a melting point of 95° C. to 125° C., and a mel
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (6)
Non-Patent Literature (5)
- "Cooler asphalt being spread in Iowa City," Aug. 16, 2011, Retrieved from "ArgusLeader.com".
- Cho et al., "A Study of Warm-Mix Asphalt's Bonding Properties on the Change of Aggregate Mineral Type and Temperature Under Thin Film Thickness," International Conference on Highway Engineering, Apr. 2012, pp. 499-503.
- Hermiston, "Eco-friendly asphalt to be used in Iowa City," Iowa City Press-Citizen, Aug. 16, 2011, pp. 1-2.
- Hurley et al., "Evaluation of SASOBIT® for Use in Warm Mix Asphalt" NCAT Report 05-06, National Center for Asphalt Technology Auburn University, 277 Technology Parkway Auburn, AL 36830, pub date, Jun. 2005.
- KCRG-TV9 ABC News, "Iowa City to Lay 'Green' Asphalt," Aug. 16, 2011, Retrieved from "http://www.kcrg.com/news/local/Iowa-City-to-Lay-Green-Asphalt-127824643.html".